24 February 2022 in Water Science & Technology
To analyze the effect of flow characteristics on electrochemical water softening, characteristics of flow fields in the vicinity of vertical plate electrodes in a bench-scale electrolysis cell for electrochemical water softening were visualized using particle image velocimetry technology, and the hardness drop values under different process conditions were measured. Properly increasing the current density or reducing the electrode spacing can increase the average flow velocity in the electrode gap. Excessive current density will cause bubble accumulation, form a bubble vortex, interfere with the orderly flow of surrounding liquid and reduce mass transfer efficiency. When the electrode spacing is 120 mm, the highest water softening efficiency measured at the current density of 60 A/m2 is 16.56%. When the current density is 50 A/m2, the highest average speed measured at the electrode spacing of 60 mm is 0.00169 m/s, but the highest water softening efficiency measured at the electrode spacing of 90 mm is 23.3%.The circulation efficiency in the electrode gap of a semi-closed structure is lower than that of a free convection structure. The behavior of bubbles is the key to flow and mass transfer. It is important to consider its influence on bubble behavior when optimizing electrochemical parameters.
1 January 2024 in International Journal of Polymer Science
To investigate the influence of acid‐base environments on the properties of chopped fiber‐reinforced resin matrix composites, corresponding unsealed specimens were prepared. These specimens were immersed in sodium hydroxide, hydrochloric acid solution, and deionized water for varying durations, after which their mechanical properties and surface hardness were tested. Changes in chemical composition, as well as alterations in fiber and resin matrix, were observed from a microscopic perspective. The results indicate that fracture at the fiber/matrix interface and hydrolysis aging of the matrix are the primary reasons for degradation in the mechanical properties of the composite. After 28 days of immersion, the hardness retention rates were found to be 54.34%, 75.96%, and 74.15% for deionized water, NaOH solution, and HCl solution, respectively. Similarly, the retention rates of tensile strength were 56.99%, 51.97%, and 58.32%, respectively. These findings provide valuable insights for the application of chopped fiber‐reinforced vinyl ester resin matrix composite materials in equipment designed in acid‐base environments.