1 November 2016 in Scripta Materialia
Coherently grown nanolayered TiN/CrN thin films exhibit a superlattice effect in fracture toughness, similar to the reported effect in indentation hardness. We found –by employing in-situ micromechanical cantilever bending tests on free-standing TiN/CrN superlattice films– that the fracture toughness increases with decreasing bilayer period (Λ), reaching a maximum at Λ~6nm. For ultrathin layers (Λ~2nm), the fracture toughness drops to the lowest value due to intermixing and loss of superlattice structure. Both, fracture toughness and hardness peak for similar bilayer periods of TiN/CrN superlattices
28 November 2017 in Scientific Reports
Hard coatings used to protect engineering components from external loads and harsh environments should ideally be strong and tough. Here we study the fracture toughness, KIC, of Ti1−xAlxN upon annealing by employing micro-fracture experiments on freestanding films. We found that KIC increases by about 11% when annealing the samples at 900 °C, because the decomposition of the supersaturated matrix leads to the formation of nanometer-sized domains, precipitation of hexagonal-structured B4 AlN (with their significantly larger specific volume), formation of stacking faults, and nano-twins. In contrast, for TiN, where no decomposition processes and formation of nanometer-sized domains can be initiated by an annealing treatment, the fracture toughness KIC remains roughly constant when annealed above the film deposition temperature. As the increase in KIC found for Ti1−xAlxN upon annealing is within statistical errors, we carried out complementary cube corner nanoindentation experiments, which clearly show reduced (or even impeded) crack formation for annealed Ti1−xAlxN as compared with their as-deposited counterpart. The ability of Ti1−xAlxN to maintain and even increase the fracture toughness up to high temperatures in combination with the concomitant age hardening effects and excellent oxidation resistance contributes to the success of this type of coatings.
1 June 2019 in Acta Materialia
5 November 2014 in Physical Review B
The dynamical and thermodynamic phase stabilities of the stoichiometric compound CrN including different structural and magnetic configurations are comprehensively investigated using a first-principles density functional theory (DFT) plus () approach in conjunction with experimental measurements of the thermal expansion. Comparing DFT and results with experimental data reveals that the treatment of electron correlations using methods beyond standard DFT is crucial. The nonmagnetic face-centered cubic B1-CrN phase is both elastically and dynamically unstable, even under high pressure, while CrN phases with nonzero local magnetic moments are predicted to be dynamically stable within the framework of the scheme. Furthermore, the impact of different treatments for the exchange-correlation (xc)-functional is investigated by carrying out all computations employing the local density approximation and generalized gradient approximation. To address finite-temperature properties, both magnetic and vibrational contributions to the free energy have been computed employing our recently developed spin-space averaging method. The calculated phase transition temperature between low-temperature antiferromagnetic and high-temperature paramagnetic (PM) CrN variants is in excellent agreement with experimental values and reveals the strong impact of the choice of the xc-functional. The temperature-dependent linear thermal expansion coefficient of CrN is experimentally determined by the wafer curvature method from a reactive magnetron sputter deposited single-phase B1-CrN thin film with dense film morphology. A good agreement is found between experimental and ab initio calculated linear thermal expansion coefficients of PM B1-CrN. Other thermodynamic properties, such as the specific heat capacity, have been computed as well and compared to previous experimental data.
1 November 2012 in Scripta Materialia
1 October 2011 in Acta Materialia