The enhancement of structural anisotropy and magnetic anisotropy in ferrite films, Fe3−xMxO4 (M = Fe, Co, Mn), which were deposited on glass substrates from aqueous solutions by thin liquid film (TLF) method at a low temperature (358 K), was compared in x-ray diffraction, conversion electron Mössbauer spectroscopy, and vibrating sample magnetometer measurements. The experimental results showed that the highly coercive Fe3−xCoxO4 films, maximum coercivity of 0.21 T at room temperature, have a preferential growing direction along the magnetic easy axis of the magnetite, 111 . While anisotropy was enhanced by the addition of Co2+ ions in the reaction solution, no enhancement was observed in the TLF-films of Fe3O4 and Fe3−xMnxO4. The enhanced anisotropy is probably caused by the extra stabilization energy of the Co2+ ions in the octahedral sites of the spinel and the interactions between the Co2+ ions in the spinel. The alternating deposition of metal ions and oxide ions in TLF process, which is a simulation of the atomic layer deposition, may help the alignment. The most anisotropic TLF film was Fe2.59Co0.41O4.
Gold nanotubes/nanoparticles are synthesized by two-step thermal decomposition of infiltrated into anodized aluminum oxide (AAO) membrane without any catalysts, reducing agents, or surfactants. The Au nanotubes deposited in AAO nanochannel ( in diameter) are composed of single crystalline Au nanoparticles ( in diameter). The Au nanotubes are electrically conducting with an apparent electrical resistivity of , which was about times larger than that of the bulk metal, , at room temperature.