Valdek Mikli

Valdek Mikli

Auto-generated profile, based on publicly available information

Valdek Mikli

Department of Materials and Environmental Technology, Tallinn University of Technology, Ehitajate tee 5, 19086 Tallinn, Estonia

Research Focus & Metrics

Academic Career Length

31Years (1996-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
20 November 2001 in Proceedings of the Estonian Academy of Sciences. Engineering
Verified
Journal Article
Open access
VMValdek Mikli
Valdek Mikli
HKHelmo Käerdi
Helmo Käerdi
PKPriit Kulu
Priit Kulu
MBMichal Besterci
Michal Besterci

1 April 2022 in Journal of Physics: Energy
Verified
Journal Article
Open access
MKM Kauk-Kuusik
M Kauk-Kuusik
KTK Timmo
K Timmo
KMK Muska
K Muska
MPM Pilvet
M Pilvet
JKJ Krustok
J Krustok
MGM Grossberg-Kuusk
M Grossberg-Kuusk
The power conversion efficiency of Cu2ZnSnS4 (CZTS) solar cells is still limited by deep defects, low minority carrier lifetime and high recombination rates at the CZTS/CdS interface. The objective of this study was to find an effective method to reduce interface recombination of CZTS monograin layer solar cells. A two-step heterojunction formation process was applied by controlling the intermixing of Cd and Cu in the CZTS/CdS interface, which resulted in improved device efficiency of up to 11.7%. Surface analysis by x-ray photoelectron spectroscopy confirmed Cd diffusion into the surface of CZTS after CdS air-annealing by forming an ultra-thin Cu2Zn x Cd1−x SnS4 layer. Moreover, external quantum efficiency measurements showed that the absorption edge shifts to longer wavelengths with the addition of Cd into the CZTS surface layer. This surface modification and replacement of a CdS:Cu buffer layer by fresh CdS greatly reduced the interface recombination and improved the junction quality, contributing to an enhancement of J SC ∼3 mA cm−2 (from 20.5 to 23.6 mA cm−2) and fill factor ∼14% (from 59.4% to 67.7%). The serial resistance of the CZTS monograin layer solar cells was significantly reduced from 2.4 Ω cm2 to 0.67 Ω cm2. To understand the electrical behavior of the highest-efficiency CZTS monograin layer solar cell in more detail, the temperature-dependent current–voltage characteristics were analyzed.

7 March 2016 in Proceedings of the Estonian Academy of Sciences
Verified
Journal Article
Open access
SSSirli Sepper
Sirli Sepper
PPPriidu Peetsalu
Priidu Peetsalu
PKPriit Kulu
Priit Kulu
MSMart Saarna
Mart Saarna
VMValdek Mikli
Valdek Mikli
The study focuses on the role of silicon in the hot dip galvanizing process. Coating formation and growth were analysed. Centrifugal casting was used to prepare steel substrates with different silicon concentrations (

5 September 2012 in Estonian Journal of Engineering
Verified
Journal Article
Open access
EAEron Adoberg
Eron Adoberg
VPVitali Podgurski
Vitali Podgurski
PPPriidu Peetsalu
Priidu Peetsalu
LLLiina Lind
Liina Lind
VMValdek Mikli
Valdek Mikli
PKPriit Kulu
Priit Kulu
Nowadays physical vapour deposited (PVD) coatings are widely used in a variety of different applications to reduce the wear of tools. Thin hard coatings have good wear resistance only when they have good adhesion and certain surface roughness. Thus, dry micro-abrasive blasting method with SiC abrasive was implemented as a pre-treatment process on WC-Co substrates. Post-treatment was conducted by using drag grinding method. The effect of surface pre- and post-treatment on the adhesion and tribological properties of TiN hard coatings have been investigated. TiN hard coatings were deposited by means of lateral rotating cathode arc method with the thickness of 2.3 µm. The surface roughness was measured by means of Mahr Perthometer and the standard Rockwell adhesion test was implemented to evaluate the adhesion of PVD TiN coatings. Tribological properties were determined by ball-on-disk method. The experimental part was focused on the effect of microblasting on the tribological properties of the coating. The relation between post-treatment of the coating and friction coefficient is indicated.

22 August 2013 in Estonian Journal of Engineering
Verified
Journal Article
Open access
ASAndrei Surzhenkov
Andrei Surzhenkov
Maksim AntonovMaksim Antonov
Maksim Antonov
DGDmitri Goljandin
Dmitri Goljandin
TVTimo Vilgo
Timo Vilgo
VMValdek Mikli
Valdek Mikli
PKPriit Kulu
Priit Kulu
In the current article, high-velocity oxy-fuel (HVOF) sprayed composite powder TiC-NiMo and Cr3C2-Ni cermet particles reinforced self-fluxing alloy matrix (FeCrSiB) coatings were studied. The actual content of the reinforcement in the sprayed coatings was smaller in comparison with the feedstock powders. Cermet particles were deformed at the impact with the substrate, deformation was more remarkable in the case of the TiC-NiMo particles. Sprayed coatings exhibited a structure with a number of defects, like voids and cracks, whereas the latter were more pronounced in reinforced coatings. Despite the bigger number of defects, cermet particles reinforced coatings had up to 1.2 times higher surface hardness than the unreinforced coating. TiC-NiMo particles reinforced coating demonstrated 1.8 times higher sliding wear resistance than the unreinforced coating. Cr3C2-Ni particles reinforced coating showed 1.3–2.8 times higher sliding wear resistance in comparison with the unreinforced coating, depending on the series of tests. Addition of cermet particles allowed to increase the resistance of the FeCrSiB matrix to deformation and scuffing.

1 February 1998 in Proceedings of the Estonian Academy of Sciences. Engineering
Verified
Journal Article
Open access
PKPriit Kulu
Priit Kulu
ATAleksei Tümanok
Aleksei Tümanok
VMValdek Mikli
Valdek Mikli
HKHelmo Käerdi
Helmo Käerdi
IKIvan Kohútek
Ivan Kohútek
MBMichal Besterci
Michal Besterci