15 October 2019 in Superconductor Science and Technology
Addition of Zn to a Cu matrix during Cu–Zn/Sn interdiffusion reactions at 400 °C leads to the formation of a solid ternary Cu–Zn–Sn phase, β -CuZn, at the outermost reaction layer next to the porous ε phase. The use of a brass matrix considerably suppresses void formation and promotes homogeneous outward Sn diffusion in pre-annealing, prior to Nb 3 Sn formation. There are exactly three paths for Ti doping in the internal tin process, i.e. doping to Sn cores, Nb filaments, and Cu matrix. Ti doping to Sn cores causes a Ti-rich layer formation at the boundary of the Nb filament pack; however, no Ti-rich layers are formed as a result of small Ti doping to the matrix and to Nb filaments. The absence of Ti-rich layers is believed to contribute to a smooth Sn diffusion and suppression of void growth. Atom probe tomography measurements reveal that Ti doping to Sn cores leads to a more inhomogeneous Ti distribution near the grain boundary and a larger variation of the grain boundary thickness than doping to Nb filaments, which may contribute to a better Sn grain boundary diffusion. It is concluded that Ti doping to the matrix, instead of doping to Sn cores, might be more effective in maintaining better growth kinetics of Nb 3 Sn.
21 January 2019 in Superconductor Science and Technology
The addition of Zn into Cu matrix has been proved to enhance the Sn activity and accelerate the formation of a Nb 3 Sn layer in internal tin-processed Nb 3 Sn wires. However, in our samples, Ti is doped in Sn cores, and during the reaction, Ti was observed to accumulate between the inner and outer sub-elements of the 1980-Nb-core multi-filamentary brass matrix wires. With the addition of Mg into the brass matrix, Ti accumulation between the sub-elements was significantly suppressed, which promoted Ti incorporation into the Nb 3 Sn layers. Meanwhile, the formed Nb 3 Sn layers exhibited smaller grain sizes. Compared to the brass (Cu-12wt%Zn) matrix wires, an improvement of critical current density ( J
c
) was found in the Cu-12Zn-0.2Mg matrix wires due to the incorporation of Ti into the Nb 3 Sn layer and the refinement of the Nb 3 Sn grain size. The irreversibility field ( B
irr
) and maximum bulk pinning forces ( F
p
,max
) were calculated from the Kramer plot by analyzing the J c ( B ) curves. A small amount of Mg (0.2 wt%) doping into the Cu-12Zn matrix wires can increase the B
irr
value by about 0.5 T and the F
p
,max
value by about 3 ∼ 4 GN m −3 after the wires were heat treated between 670 °C and 730 °C. The non-Cu J
c
of the Cu-12Zn-0.2Mg matrix wires reaches the maximum value of 1533 A mm −2 @12 T after heat treatment at 685 °C and decreases at higher temperatures.
1 September 2019 in Materials Today Communications
1 April 2021 in Intermetallics
13 July 2023 in Superconductor Science and Technology
Due to the limited available piece length of YBCO-coated conductors (i.e. tapes or wires) and the different requirements for magnetic field, joints are inevitable for manufacturing high-temperature superconducting magnets. In this study, a sintering nano-silver (Ag) process was developed and used to connect YBCO tapes stabilized by anAg layer with low-temperature and short-time sintering of Ag nanoparticle (NP) paste. The thermodynamic characteristics of Ag NP paste were explored using a TG/DSC setup. The effects of sintering temperature, mechanical pressure and lapped length on microstructures and electrical properties of joints were comprehensively investigated. It is found that the pre-volatilization of low-boiling-point solvent in the paste is beneficial to improve the densification of sintered structure, thus contributing to increasing the critical current I c of the joint. With increasing sintering temperature, the I c of the joint will be close to that of the virgin tape, and the joint resistance experiences small fluctuations, but joint connectivity is enhanced. As the temperature reaches 205 °C, I c decreases to 84% of the virgin tape, and joint resistance increases obviously. In addition, the axial tension strength at room temperature is improved with the increase in mechanical pressure, while the resistance does not demonstrate distinct variation. Considering the electromechanical properties, the optimal joining process is determined as sintering at 180 °C and 30 MPa for 10 min. The joint with this technology possesses a closely connected interface and a well-sintered nano-Ag microstructure with pores. By further extending the lapped length, a YBCO joint resistivity as low as ∼10.56 nΩ cm2 is obtained, which is around a quarter of that of the soldering joint, and the process is much easier than that of the Ag diffusion joint.
1 September 2019 in Journal of Alloys and Compounds