Shunsuke Muto

Shunsuke Muto

Auto-generated profile, based on publicly available information

Shunsuke Muto

Department of Materials Physics, Graduate School of Engineering, Nagoya University , Furo-cho, Chikusa-ku, Nagoya 464-8603

Research Focus & Metrics

Academic Career Length

40Years (1987-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
24 April 2011 in Nature
Verified
Journal Article
Closed access
RNRyuichi Nomura
Ryuichi Nomura
HOHaruka Ozawa
Haruka Ozawa
STShigehiko Tateno
Shigehiko Tateno
KHKei Hirose
Kei Hirose
JHJohn Hernlund
John Hernlund
NHNozomu Hiraoka
Nozomu Hiraoka

1 January 2009 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
SMShunsuke Muto
Shunsuke Muto
YSYusuke Sasano
Yusuke Sasano
KTKazuyoshi Tatsumi
Kazuyoshi Tatsumi
TSTsuyoshi Sasaki
Tsuyoshi Sasaki
KHKayo Horibuchi
Kayo Horibuchi
YUYoshio Ukyo
Yoshio Ukyo
We used a suite of transmission electron microscopy (TEM) and associated electron spectroscopy methods to examine the local structure and changes in the electronic structure of positive electrode material. We found a scattered rock-salt phase near grain surfaces and grain boundaries, where turned to , deduced from relative intensity ratios and fine structures of the white-line peaks of the transition metals. The spatial distribution of the degraded phase throughout the secondary particle was found using a scanning TEM-electron energy loss spectroscopy spectral imaging technique and multivariate analysis. The degradation process and its relationship to the surface reactions with electrolytes is discussed based on the spatial-distribution map of the degraded phases.

4 September 2000 in Applied Physics Letters
Verified
Journal Article
Closed access
PDF file
TKTomoyuki Kakeshita
Tomoyuki Kakeshita
TTTetsuya Takeuchi
Tetsuya Takeuchi
TFTakashi Fukuda
Takashi Fukuda
MTMasato Tsujiguchi
Masato Tsujiguchi
TSToshio Saburi
Toshio Saburi
SMShunsuke Muto
Shunsuke Muto
Magnetostriction measurements have been made in an ordered Fe3Pt single crystal with degree of order of about 0.8, which exhibits a cubic-tetragonal martensitic transformation at 97 K. The specimen was cooled down to 4.2 K without magnetic field, and then a magnetic field of 4 T is applied to the specimen along 〈001〉 at 4.2 K and removed. As a result, a reversible giant magnetostriction of about 0.5% is observed. This reversible magnetostriction will be caused by the rearrangement of crystallographic domains, being three times as large as that of Terfenol-D (Fe2DyxTb1−x: typical magnetostrictive materials).

1 October 1992 in Chemical Physics
Verified
Journal Article
Closed access
MVM.A. Verheijen
M.A. Verheijen
HMH. Meekes
H. Meekes
GMG. Meijer
G. Meijer
PBP. Bennema
P. Bennema
JBJ.L. de Boer
J.L. de Boer
JLJ. van Landuyt
J. van Landuyt

23 October 2019 in Nature Communications
Verified
Journal Article
Open access
PDF file
ZZZhujun Zhang
Zhujun Zhang
IKIzuru Karimata
Izuru Karimata
HNHiroki Nagashima
Hiroki Nagashima
SMShunsuke Muto
Shunsuke Muto
KOKoji Ohara
Koji Ohara
TTTakashi Tachikawa
Takashi Tachikawa
Hematite (α-Fe2O3) is one of the most promising candidates as a photoanode materials for solar water splitting. Owing to the difficulty in suppressing the significant charge recombination, however, the photoelectrochemical (PEC) conversion efficiency of hematite is still far below the theoretical limit. Here we report thick hematite films (∼1500 nm) constructed by highly ordered and intimately attached hematite mesocrystals (MCs) for highly efficient PEC water oxidation. Due to the formation of abundant interfacial oxygen vacancies yielding a high carrier density of ∼1020 cm−3 and the resulting extremely large proportion of depletion regions with short depletion widths (<10 nm) in hierarchical structures, charge separation and collection efficiencies could be markedly improved. Moreover, it was found that long-lived charges are generated via excitation by shorter wavelength light (below ∼500 nm), thus enabling long-range hole transfer through the MC network to drive high efficiency of light-to-energy conversion under back illumination.

1 January 2009 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
TSTsuyoshi Sasaki
Tsuyoshi Sasaki
TNTakamasa Nonaka
Takamasa Nonaka
HOHideaki Oka
Hideaki Oka
COChikaaki Okuda
Chikaaki Okuda
YIYuichi Itou
Yuichi Itou
SMShunsuke Muto
Shunsuke Muto
The mechanism for capacity fade of lithium-ion batteries with <mml:math display="inline"><mml:mrow><mml:mi mathvariant="normal">Li</mml:mi><mml:msub><mml:mi mathvariant="normal">Ni</mml:mi><mml:mrow><mml:mn>0.8</mml:mn></mml:mrow></mml:msub><mml:msub><mml:mi mathvariant="normal">Co</mml:mi><mml:mrow><mml:mn>0.15</mml:mn></mml:mrow></mml:msub><mml:msub><mml:mi mathvariant="normal">Al</mml:mi><mml:mrow><mml:mn>0.05</mml:mn></mml:mrow></mml:msub><mml:msub><mml:mi mathvariant="normal">O</mml:mi><mml:mrow><mml:mn>2</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math>LiNi0.8Co0.15Al0.05O2 as a positive electrode material associated with cycling at elevated temperatures was investigated by the combination of electrochemical and spectroscopic methods. The total capacity fade of the battery after charge/discharge cycle test at <mml:math display="inline"><mml:mrow><mml:mn>80</mml:mn><mml:mo>°</mml:mo><mml:mi mathvariant="normal">C</mml:mi></mml:mrow></mml:math>80°C was found to be almost explained by the capacity fade of the positive electrode, which indicates that the degradation of the positive electrode is mainly responsible for capacity fade of the battery at this temperature. Quantitative analyses revealed a strong positive correlation between the capacity fade of the positive electrode and the amount of inactive Ni ions in the active material after the cycling test. It is concluded that the capacity fade is mainly caused by the formation of inactive Ni(II) and Ni(III), presumably associated with oxygen loss in the active materials, which act as obstacles to Li intercalation/deintercalation.