Ca2Al2SiO7 (CAS) bulk single crystals were grown by the Czochralski method. Material constants of the crystal were determined over the driving temperature range of a typical combustion pressure sensor. The electrical resistivity at 800 °C was found to be of the order of 108 Ωcm. We constructed a measurement system for the direct piezoelectric effect at high temperature, and characterized the crystals in a simulated engine cylinder combustion environment. Output charge signal against applied stress was detected at 700 °C. These observations suggest that CAS crystals are superior candidate materials for high temperature for stress sensing.
Dense and phase-pure (Bi1/2K1/2)TiO3 (BKT) ceramics with various average grain sizes from 0.18 to 1.01 μm were prepared from a hydrothermally synthesized powder and their phase transition behaviors were studied by means of dielectric measurements. A drastic increase of the maximum dielectric permittivity (εm) with increasing the grain size was found in the temperature dependence of permittivity. The sample with the largest grain size clearly showed both a frequency dependence of dielectric maximum temperature (Tm) and a dielectric anomaly with a strong thermal hysteresis at a temperature below Tm, demonstrating that the BKT ceramic is intrinsically a material exhibiting a spontaneous relaxor to normal ferroelectric (R-nFE) phase transition. On the other hand, the suppression of the R-nFE transition was observed in the sample with the smallest grain size, which was explained as an effect of avoiding the internal stress development caused by the volume increase occurring with the phase transition.
The temperature evolution of polar order in an -site complex perovskite (BKT) has been investigated by measurements of dielectric permittivity, depolarization current, and stress-stain curves at elevated temperatures. Upon cooling from high temperatures, BKT first enters a relaxor state and then spontaneously transforms into a ferroelectric state. The analyses of temperature and frequency dependence of permittivity have revealed that polar nanoregions of the relaxor phase appear at temperatures higher than , and also that their freezing at triggers the spontaneous relaxor-ferroelectric transition. We discuss the key factors determining the development of long-range polar order in -site complex perovskites through a comparison with the relaxor . We also show that application of biasing electric fields and compressive stresses to BKT favors its ferroelectric phase, resulting in a significant shift of the relaxor-ferroelectric transition temperature towards higher temperatures. Based on the obtained results, electric field-temperature and stress-temperature phase diagrams are firstly determined for BKT.
Dense and phase-pure (Bi 1/2 K 1/2 )TiO 3 (BKT) ceramics with various grain sizes from 0.18 to 1.01 µm were prepared by conventional sintering of a hydrothermally synthesized fine powder. The decrease in grain size resulted in the reductions in tetragonality, remanent polarization, and the piezoelectric d33 coefficient, whereas the room-temperature dielectric permittivity slightly increased with decreasing grain size. The measurement of the temperature dependence of permittivity revealed that BKT exhibited the spontaneous relaxor-to-normal ferroelectric (R-nFE) phase transition. It was also found that the maximum permittivity was decreased and the R-nFE transition was inhibited by the reduction in grain size. In this paper, on the basis of the observed grain-size-dependent phase transition behaviors, microstructural models are proposed for both coarse- and fine-grained BKT ceramics, and the mechanism underlying the grain size effect on the electrical properties is discussed.
We have proposed a fabrication process of submicrometer-sized zinc oxide aggregates with nano/microstructures through pyrolysis of ZIF-8 particles. Methanol solutions of zinc nitrate hexahydrate and 2-methylimidazole were used for synthesizing ZIF-8 with its characteristic rhombic dodecahedron morphology. The systematic addition of 1-methylimidazole to the above methanol solutions led to the formation of size-tunable ZIF-8 particles. Precise control of heating conditions was a key to successful conversion from ZIF-8 to ZnO without destroying the morphology. The ZnO aggregates thus obtained were evaluated as photoanode materials of dye-sensitized solar cells. A photoanode using a 9 μm thick ZnO aggregate film gave a power conversion efficiency of 3.37% due to its nano/microstructures being suitable for dye adsorption, electrolyte diffusion, and light harvesting.