15 April 2024 in Powder Metallurgy аnd Functional Coatings
The paper presents the results of theoretical and experimental studies regarding the quality of diffusion welding of the beryllium–copper composite. Numerical investigations of the parameters of heterodiffusion of diffusants and the thickness of the Be–Cu pair welded joint under varying temperature-time conditions were conducted. The analytical examinations revealed that the thickness of the diffusion weld at the Be–Cu joint varies between 26 and 345 µm, with the temperature increasing from 800 to 1000 °C and the holding time ranging from 20 to 120 min. The calculated layer thickness during the diffusion welding of a Be–Cu pair at 800 °C for 2 h is 65 µm, with 15 µm on the beryllium side and 50 µm on the copper side. Notably, a CuBe3 intermetallic compound zone can form in the diffusion weld, which should be considered an adverse factor that reduces the mechanical properties. To theoretically substantiate the modification of the structure and properties of the diffusion zone, a numerical study of welding was carried out using a 10 μm thick nickel foil spacer, which is readily soluble in beryllium. It was demonstrated that after exposure to temperature-time conditions at 900 °C for 20 min, a 50 µm wide diffusion-bonded joint is formed. Its structure includes two single-phase zones of solid solutions based on copper and beryllium, as well as two two-phase regions consisting of solid solutions hardened with intermetallic compounds. Since the weld lacks structural zones consisting solely of intermetallic compounds (unlike when welding the Be–Cu diffusion pair), there are grounds to anticipate a reduction in the embrittling effect on the weld. The results obtained from the analytical studies can serve as the foundation for a theoretical prediction method for assessing the quality of diffusion welding of the beryllium–copper composite.
29 December 2023 in Powder Metallurgy аnd Functional Coatings
Experimental and analytical studies on gas atomization of the molten beryllium and the production of beryllium granules are presented. The impact of various factors, including the choice of gas (nitrogen or helium), the cooling gas flow rate (ranging from 300 to 650 m/s), melt temperature, and droplet size (<500 µm), on the cooling rate and granule properties, is demonstrated. It has been determined that the solidification of beryllium granules can occur through two distinct mechanisms depending on the atomization process. These mechanisms include crystallization and amorphization (glass transition). When beryllium melt is atomized with nitrogen, granules with diameters less than 100 µm solidify via the amorphization mechanism (glass transition), while those with diameters exceeding 300 µm solidify through crystallization. In such cases, a portion of granules with sizes ranging from 100 to 300 µm undergoes a mixed mechanism solidification. In this process, the surface becomes amorphous, while the central part crystallizes, resulting in the formation of a “shell” on the surface, marking the transition from the glass transition mechanism to the crystallization mechanism. The thickness of this “shell” depends on the granule diameter, measuring 10–15 µm for 300 µm granules and 20–25 µm for 100 µm granules. The findings from this research align well with the hypothesis of a glass-crystalline mechanism of beryllium granule solidification, which leads to their separation at the interfacial boundary. Such solidification through a mixed mechanism results in the creation of a removable “crust” on the granule, which is typically more contaminated with impurities. Understanding this effect opens up possibilities for practical applications in the production of specialized materials from beryllium. The ability to separate the “crust” from the “core” provides the conditions for obtaining specialized sintered beryllium grades suitable for use in nuclear reactors and foil production, where a beryllium microstructure with “clean” boundaries is essential.