Currently, the use of biodegradable polymers for packaging application has been an imperative topic due to the environmental damage caused by non-biodegradable materials. In the present study, PBAT/ZnO biodegradable nanocomposites were prepared by melt processing and characterized by FEG-SEM, DSC, XRD, TDNMR and water activity analysis. The main results showed an increase in the Tc values for all produced formulations, indicating a change in the crystalline profile of the PBAT, which was corroborated by XRD results. FEG-SEM showed that the systems containing up to 1 wt.% of ZnO showed better nanoparticles dispersion, while formulations containing 3 and 5 wt.% of ZnO presented large aggregates. TDNMR provided a more detailed assessment, showing that PBAT/ZnO systems containing 0.5 and 5 wt.% of ZnO presented a higher heterogeneity at molecular level. Finally, water activity analysis showed that ZnO addition promoted an increment in the biosafety levels compared to neat PBAT, making the PBAT/ZnO nanocomposites more promising for food packaging application.
1 January 2025 in Anais da Academia Brasileira de Ciências
The persistent accumulation of microplastics from synthetic polymers threatens ecosystems and biodiversity. The use of biodegradable and compostable materials as alternatives to conventional plastics in food packaging has shown promise, particularly with the development of nanocomposites that can be tailored to meet market demands. In this study, ZnO and TiO₂ nanoparticles were combined and incorporated into a biodegradable poly(butylene adipate-co-terephthalate) (PBAT) matrix at varying concentrations, forming a novel ternary PBAT/ZnO/TiO₂ system. The films produced via melt processing were characterized using conventional and non-conventional techniques to evaluate their thermal, morphological, chemical, wettability, and biosafety properties. The results indicated that the combined addition of ZnO and TiO₂ slightly reduced the thermal stability and crystallinity of PBAT, while increasing surface hydrophilicity. These features may contribute to accelerated degradation and reduced environmental persistence. Furthermore, improvements in the elastic modulus and enhanced biosafety were observed across all tested concentrations. These findings suggest that the prepared nanocomposites, particularly at 0.75 and 1 wt%, not only possess properties suitable for food packaging applications but also demonstrate potential to mitigate environmental persistence through accelerated degradation. Therefore, this study supports the development of environmentally friendly materials for food packaging, addressing the urgent need to reduce microplastic pollution.