This study develops a silica-reinforced Inconel 718 nanocomposite fabricated by laser powder bed fusion (LPBF) and heat treated according to AMS 5663. The composite processing window was examined by varying volumetric energy density from -30% to +30% relative to the optimized monolithic Inconel 718 condition. Adding only 1 wt.% nano-SiO₂ and increasing the energy density by 10% produced near-fully dense specimens (99.9% relative density), reduced porosity, weakened the ∥build direction texture, and promoted a refined, partially equiaxed grain structure. XRD, EBSD, and TEM/EDS analyses revealed in-situ formation of thermally stable nanoscale Al–Ti oxides and Nb-silicides (≈50–100 nm), which pin grain/subgrain boundaries after heat treatment. These microstructural changes enhanced high-temperature tensile properties at 650 °C, giving a yield strength of 940 ± 25 MPa, UTS of 1128 ± 18 MPa, and elongation of 10.5 ± 1%, exceeding heat-treated monolithic LPBF Inconel 718. Creep testing at 650 °C/650 MPa showed retained rupture life (30 ± 4 h) while rupture elongation increased from 1.7% to 4.7%. The improvement is attributed to defect suppression, grain-boundary stabilization, Orowan strengthening, CTE-mismatch, and limited load transfer.
Achieving simultaneous high strength and ductility remains a fundamental limitation in structural alloys. Fe–Cu systems offer substantial strengthening potential via precipitation, but their development is severely constrained by immiscibility and pronounced Cu segregation during solidification. Here, we demonstrate that laser powder bed fusion (LPBF) provides a nonequilibrium processing route that overcomes these limitations by enabling in situ homogenisation and ageing through rapid thermal cycling. This results in a homogeneous dispersion of coherent, nanoscale (2–5 nm) Cu precipitates within the Fe matrix without any post-processing. The alloy containing 4.5 wt.% Cu exhibits the best combination of strength and ductility, with a lower and upper yield strength of 920 MPa and ~1000 MPa, respectively, while retaining high elongation-to-failure (up to 27%) and nearly unchanged uniform elongation (~11–12%) compared with pure Fe. A similar strength-ductility synergy is exhibited by Fe–3 wt.% Cu, with a lower yield strength of ~670 MPa and elongation-to-failure of up to 32%, thereby pushing the boundary of the conventional strength–ductility trade-off. Microstructural and analytical evidence reveal that closely spaced, shearable Cu precipitates enable uniform dislocation activity and suppress strain localisation. Their size distribution coincides with the theoretically optimal regime for precipitation strengthening, indicating that the alloy approaches the upper limit of achievable strengthening. These findings establish LPBF as a powerful route for designing high-performance immiscible alloys.
In this study, the influence of deposition sequence on the interfacial microstructure, porosity, hardness, and thermal conductivity of Inconel 718 (IN718)-Cu and IN718-GRCop-42 multi-material joints fabricated via Cold Spray Additive Manufacturing (CSAM) was systematically investigated. Thermal conductivity was evaluated in the in-plane direction using the Transient Plane Source (TPS) method and in the through-plane direction using Laser Flash Analysis (LFA) . The Cu/ IN718 multi-material exhibited the highest in-plane thermal conductivity, approximately 170 W/m·K, because interfacial resistance has a much smaller effect on heat flow parallel to the interface than on heat flow across the interface. In contrast, the through-plane thermal conductivity of all multi-material samples was significantly lower, reflecting the dominant role of interfacial thermal resistance in the build direction. All multi-material samples were subjected to aging treatment (720 °C for 8 h followed by 620 °C for 8 h in a controlled atmosphere). Following heat treatment, the GRCop-42-IN718 samples exhibited a marked enhancement. This improvement is likely associated with microstructural evolution during thermal processing, including grain growth, homogenization, and stress relief in the Cu-rich regions. Overall, this work demonstrates that deposition sequence and post-processing heat treatment critically influence interfacial characteristics and thermal transport in CSAM-fabricated multi-material systems.
Achieving simultaneous high strength and ductility remains a fundamental limitation in structural alloys. Fe–Cu systems offer substantial strengthening potential via precipitation, but their development is severely constrained by immiscibility and pronounced Cu segregation during solidification. Here, we demonstrate that laser powder bed fusion (LPBF) provides a nonequilibrium processing route that overcomes these limitations by enabling in situ homogenisation and ageing through rapid thermal cycling. This results in a homogeneous dispersion of coherent, nanoscale (2–5 nm) Cu precipitates within the Fe matrix without any post-processing. The alloy containing 4.5 wt.% Cu exhibits the best combination of strength and ductility, with a lower and upper yield strength of 920 MPa and ~1000 MPa, respectively, while retaining high elongation-to-failure (up to 27%) and nearly unchanged uniform elongation (~11–12%) compared with pure Fe. A similar strength-ductility synergy is exhibited by Fe–3 wt.% Cu, with a lower yield strength of ~670 MPa and elongation-to-failure of up to 32%, thereby pushing the boundary of the conventional strength–ductility trade-off. Microstructural and analytical evidence reveal that closely spaced, shearable Cu precipitates enable uniform dislocation activity and suppress strain localisation. Their size distribution coincides with the theoretically optimal regime for precipitation strengthening, indicating that the alloy approaches the upper limit of achievable strengthening. These findings establish LPBF as a powerful route for designing high-performance immiscible alloys.