7 September 2010 in Smart Materials and Structures
16 August 2023 in International Journal of Solids and Structures
6 June 2022 in Journal of the Mechanics and Physics of Solids
1 July 2007 in Materials Science Forum
The aim of this study is to acquire more quantitative data on the cold-deformed state, in order to determine the key parameters for nucleation (like orientation gradient, dislocation density, degree of fragmentation…) and to correlate these to parameters which can be predicted by a mean field deformation model. Experimentally, a Ti-IF hot band has been deformed by cold rolling up to 51%. The deformed microstructures are finely characterised using EBSD inside the SEM. It appears then that the heterogeneity of deformation inside the grains begins very early. Some grains undergo fragmentation whereas some others deform very homogeneously. Misorientation and degree of fragmentation are found to be orientation and rolling level dependent. These deformation parameters are plotted against the Taylor factor, calculated in each grain.
11 March 2024 in International Journal of Solids and Structures
23 December 2024 in Metallurgical Research & Technology
The effect of pre-straining on ferrite/pearlite phase transformation in high strength steels is investigated. Two steels differing mainly in their Nb content (0.03C 0.68Si 1.82Mn 0.00 or 0.04Nb in mass%) are either pre-tensioned or pre-compressed and the same-directional transformation strain is measured. A crystal plasticity fast Fourier transform numerical model with back stress effect is used for further investigation and the results are compared. Experimentally, it was found that 30% pre-tension reduces the transformation strain in the same direction by 0.09% (0.00Nb) and 0.13% (0.04Nb), while 30% pre-compression increases it by 0.16% (0.00Nb) and 0.02% (0.04Nb). The numerical simulation estimates the experimentally observed anisotropic transformation strain. In the numerical simulation, even though the anisotropy in transformation plasticity has been qualitatively reproduced, a larger anisotropy effect was observed. The quantitative discrepancies found in between experimental results and numerical results are due to the annihilation of dislocations during the interval between the pre-straining and the onset of phase transformation. The anisotropy in transformation strain found in the experiments is large enough to cause an unacceptable dimensional change in e.g. heat treated steel sheet products.