Bacillus megaterium 314 strain was able to utilize agricultural and industrial wastes for metallo-protease production. Orange peel and wheat bran were found as the most suitable carbon and nitrogen sources, respectively. Optimized production process enhanced the enzyme production by 5.1-folds. Glass and glass-ceramic with different particle sizes based on mica were used as inorganic carrier. Protease enzyme was immobilized by covalent bonding and physical adsorption methods on nanoparticle supports. Enzyme physically adsorbed on glass ceramic (particle size 0.71-1.0 mm) had the highest residual activity and the highest immobilization yield. Glass-ceramic was characterized by X-ray diffraction (XRD) and scanning electron microscopy (SEM). Immobilized enzyme exhibited activation energy (E a ) and deactivation rate constant at 60 °C (k d ) about 1.29 and 1.46-times, respectively lower than free enzyme. Moreover, adsorbed enzyme had higher energy for denaturation (E d ), half-life (t 1/2 ), and decimal reduction time (D). The thermodynamic parameters of irreversible thermal denaturation for the protease enzyme indicate that immobilized enzyme had higher enthalpy (ΔH°), free energy (ΔG°), and entropy (ΔS°) than free one. There was a significant improvement in the maximum reaction velocity Vmax (2.5-fold), Michaelis constant Km (1.9-fold), and catalytic efficiency Vmax/Km (4.7-fold) values after immobilization indicating the efficiency and effectiveness of immobilization approach.
This work pointed out the effect of adding P2O5 and/or MnO2 on the crystallization behavior of magnetic glass ceramic in the system Fe2O3·ZnO·CaO·SiO2·B2O3. The differential thermal analysis of the quenched samples revealed decrease in the thermal effects by adding P2O5 and/or MnO2 to the base sample. The X-ray diffraction patterns show the development of nanometric magnetite crystals in a glassy matrix. Heat treatment at 800 °C for 2 h, under reducing atmosphere, caused an increase in the amount of the crystallized magnetite with the appearance of minor hematite and Ca2SiO4. The transmission electron microscope revealed a crystallite size in the range 10-30 nm. Magnetic hysteresis cycles were analyzed with a maximum applied field of 25 kOe at room temperature. The prepared magnetic glass ceramics are expected to be useful for localized treatment of cancer.