The phase‐down scenario of conventional refrigerants used in gas–vapor compressors and the demand for environmentally friendly and efficient cooling make the search for alternative technologies more important than ever. Magnetic refrigeration utilizing the magnetocaloric effect of magnetic materials could be that alternative. However, there are still several challenges to be overcome before having devices that are competitive with those based on the conventional gas–vapor technology. In this paper a rigorous assessment of the most relevant examples of 14 different magnetocaloric material families is presented and those are compared in terms of their adiabatic temperature and isothermal entropy change under cycling in magnetic‐field changes of 1 and 2 T, criticality aspects, and the amount of heat that they can transfer per cycle. The work is based on magnetic, direct thermometric, and calorimetric measurements made under similar conditions and in the same devices. Such a wide‐ranging study has not been carried out before. This data sets the basis for more advanced modeling and machine learning approaches in the near future.
Magnetic refrigeration relies on a substantial entropy change in a magnetocaloric material when a magnetic field is applied. Such entropy changes are present at first‐order magnetostructural transitions around a specific temperature at which the applied magnetic field induces a magnetostructural phase transition and causes a conventional or inverse magnetocaloric effect (MCE). First‐order magnetostructural transitions show large effects, but involve transitional hysteresis, which is a loss source that hinders the reversibility of the adiabatic temperature change ΔTad. However, reversibility is required for the efficient operation of the heat pump. Thus, it is the mastering of that hysteresis that is the key challenge to advance magnetocaloric materials. We review the origin of the large MCE and of the hysteresis in the most promising first‐order magnetocaloric materials such as Ni–Mn‐based Heusler alloys, FeRh, La(FeSi)13‐based compounds, Mn3GaC antiperovskites, and Fe2P compounds. We discuss the microscopic contributions of the entropy change, the magnetic interactions, the effect of hysteresis on the reversible MCE, and the size‐ and time‐dependence of the MCE at magnetostructural transitions.
We report on magnetocaloric properties of polymer-bonded La(Fe,Si)13 heat exchangers with respect to the grain size of the powder used and the pressure applied for compaction of plates. Quite remarkably, it was found that the values of the adiabatic temperature change of polymer-bonded plates are 10% higher than in the initial bulk material. A critical value of the pressure applied during the compaction was found. Exceeding this value leads to a drastic reduction of the magnetocaloric effect due to cracking and comminution of the initial 50–100 μm grains down to 1–10 μm fragments. Compacting the LaFe11.6Si1.4 powder with 5 wt. % of silver epoxy under an optimal pressure of 0.1 GPa resulted in the production of 0.6 mm-thick plates. These plates were subsequently stacked and glued together into a simple porous heat exchanger with straight 0.6 mm-width channels.
The influence of magnetocrystalline anisotropy on the magnetocaloric effect (MCE) was studied on single crystals of Co2B and compared to measurements on polycrystalline samples. Large differences in adiabatic temperature change ΔTad and magnetic entropy change ΔSM were found along the different crystallographic directions. The magnetocaloric effect differs by 40% in the case of ΔTad in a field change of 1.9 T when applying the field along the hard axis and easy plane of magnetization. In the case of ΔSM, the values differ 50% and 35% from each other in field changes of 1 and 1.9 T, respectively. It was found that this anisotropy effect does not saturate in fields up to 4 T, which is higher than the anisotropy field of Co2B (≈2 T). A simple model was developed to illustrate the possible effect on magnetocrystalline anisotropy, showing large differences especially in application relevant fields of about 1 T. The results strongly suggest that the MCE could be maximized when orienting single crystalline powders in an easy axis parallel to the applied field in active magnetocaloric regenerator structures, and therefore the overall device efficiency could be increased.