1 June 2021 in International Journal of Machine Tools and Manufacture
30 August 2024 in International Journal of Mechanical Sciences
31 July 2025 in Advanced Equipment
It is necessary to predict the milling performance of different metal materials. This work develops a predictive model based on theoretical similarity reasoning model to evaluate cutting energy consum...
19 August 2026 in Materials Science in Additive Manufacturing
Conventional metal-bonded diamond abrasive tools with a uniform matrix cannot simultaneously achieve mechanical strength, heat dissipation, and chip clearance. Voids improve heat dissipation and chip clearance, but they compromise structural strength. This study presents a binder jetting‑based approach for fabricating tools with a built‑in strengthening skeleton. The proposed tool integrates a binder jetting-printed 316L skeleton, diamond grains, 316L filler, and infiltrated bronze into a single composite. Binder jetting offers exceptional design freedom and precise thermal control, making it well-suited for temperature-sensitive materials. The skeleton defines the abrasive zone and overall geometry, provides structural strength, and creates channels for heat dissipation and chip removal. After packing the abrasive zone with the diamond-filler mixture, the assembly undergoes bronze infiltration at moderate temperatures to consolidate the structure. In this study, dense and structured abrasive tools with 100% abrasive concentration and uniform diamond distribution in the metal matrix were produced. Interfacial reactions between diamond and the 316L filler led to minor surface degradation, thereby enhancing mechanical interlocking at the diamond-matrix interface. The three-point bending strength of dense specimens increased with bronze content, reaching 350–400 MPa. Grinding tests using SS304 as the workpiece confirmed the effectiveness of the proposed fabrication route.
18 April 2026 in SSRN Electronic Journal
The ceramic material Silicon carbide (SiC) has significant potential for applications in stereolithography apparatus (SLA) manufacturing technology. Nevertheless, SiC ceramic composites are severely limited in their applications due to their high absorption. In this paper, a surface modification process for the sol-gel method is discussed. The Al2O3 coating layer was successfully coated on the surface of SiC particles and the effect of alumina coating amount on the material properties was systematically investigated. By combining Bruggeman's effective medium theory model analysis, the regulation mechanism of the coating layer on its light scattering behavior was verified. Experimental and model analysis demonstrated that the Al2O3 coating effectively reduces the absorbance and viscosity of SiC ceramic materials while significantly enhancing the curing thickness and solids content of the ceramic slurry through the SLA process. Both the theoretical model and experimental data showed a consistent decrease in the extinction coefficient, confirming the coating layer's inhibitory effect on light absorption. When the solid content of the ceramic slurry was 72 wt%, the viscosity of the slurry was 0.84 Pa·s (shear rate of 30 s-1), and the curing thickness of the monolayer was 153 ± 10 μm. The final SiC ceramic composites, with a density of 2.67 g/cm3 and an average flexural strength of 44.7 ± 1.9 MPa, were obtained after degreasing and sintering. In this research, a novel approach is developed for the broad application of non-oxide ceramic composites, such as SiC fabricated by SLA, thereby paving the way for their expanded use.