Ethylenediaminetetraacetic acid (EDTA) is commonly used during the preparation of obstructed root canals that face a high risk of root perforation. Such perforations may be repaired with mineral trioxide aggregate (MTA). Due to EDTA’s ability to chelate calcium ions, we hypothesized that EDTA may disrupt the hydration of MTA. Using scanning electron microscopy and energy-dispersive x-ray spectroscopy, we found that MTA specimens stored in an EDTA solution had no crystalline structure and a Ca/Si molar ratio considerably lower than those obtained for specimens stored in distilled water and normal saline. Poor cell adhesion in EDTA-treated MTA was also noted. X-ray diffraction indicated that the peak corresponding to portlandite, which is normally present in hydrated MTA, was not shown in the EDTA group. The microhardness of EDTA-treated specimens was also significantly reduced (p < 0.0001). These findings suggest that EDTA interferes with the hydration of MTA, resulting in decreased hardness and poor biocompatibility.
1 January 2018 in International Journal of Nanomedicine
Mineral trioxide aggregate (MTA) is the most frequently used repair material in endodontics, but the long setting time and reduced mechanical strength in acidic environments are major shortcomings. In this study, a novel sol-gel-derived calcium silicate cement (sCSC) was developed using an initial Ca/Si molar ratio of 3, with the most effective mixing orders of reactants and optimal HNO3 catalyst volumes. A Fourier transform infrared spectrometer, scanning electron microscope with energy-dispersive X-ray spectroscopy, and X-ray powder diffractometer were used for material characterization. The setting time, compressive strength, and microhardness of sCSC after hydration in neutral and pH 5 environments were compared with that of MTA. Results showed that sCSC demonstrated porous microstructures with a setting time of ~30 min, and the major components of sCSC were tricalcium silicate, dicalcium silicate, and calcium oxide. The optimal formula of sCSC was sn200, which exhibited significantly higher compressive strength and microhardness than MTA, irrespective of neutral or pH 5 environments. In addition, both sn200 and MTA demonstrated good biocompatibility because cell viability was similar to that of the control. These findings suggest that sn200 merits further clinical study for potential application in endodontic repair of perforations.