Thermally driven oxygen production using oxygen storage materials (OSM) represents a promising alternative to conventional electrically driven air separation technologies, particularly for applications with available industrial waste heat. In this study, oxygen production using 380 g of Ba0.5Sr0.5Co0.8Fe0.2O3-δ (BSCF 5582) mini-honeycombs per packed-bed in a cyclic process with steam as sweep gas was experimentally investigated. The developed experimental setup enabled alternating oxygen adsorption and desorption cycles at furnace temperatures between 600 and 900 °C using preheated air and steam. The influence of the furnace temperature, steam mass flow rate, air flow rate and cycle duration on the oxygen production behavior was evaluated. Increasing the furnace temperature resulted in higher oxygen yields, with a maximum yield of approximately 0.85 L at standard temperature and pressure per 6-minute cycle at 900 °C and oxygen purities between 91 and 95 vol%. Across all investigated temperatures, approximately 90 % of the total oxygen yield was released within the first 3.5 minutes of each cycle. Consequently, reducing the cycle duration from 6 minutes to 3.5 minutes resulted in only a minor decrease in oxygen yield while increasing the hourly oxygen production by approximately 50 %.,The desorption behavior was analyzed using the pseudo-second-order kinetic model, which described the experimental data with a median coefficient of determination of 0.9897. Durability investigations over 302 h showed that the BSCF 5582 mini-honeycombs remained structurally intact under high-temperature steam exposure. Overall, the results demonstrate the high potential of BSCF 5582 mini-honeycombs for decentralized oxygen production using industrial waste heat.