The swelling, microstructure, and composition of grain boundaries in neutron-irradiated V–Fe alloys has been studied. It has been established that the swelling of V–Fe alloys observed after irradiation at a temperature of 370°С to a damaging dose of 1.3 dpa continuously decreases with an increase in the iron concentration from 0.7 to 5 at %. It is shown that at the grain boundaries in the V–2Fe and V–5Fe alloys an increased iron content is observed.
In gas-bonded fuel pins the interior space is filled with helium in order to provide heat removal from the fuel. Under irradiation, as a result of gaseous fission products release, the initial gas composition under the fuel pin cladding changes, which leads to a change in its thermophysical characteristics. Post-irradiation examinations have shown that the partial pressure of nitrogen under the fuel pin cladding increases with fuel burn-up increase, since nitrogen atoms also release from uranium-plutonium nitride fuel under the cladding, in addition to the krypton, xenon and helium inert gases. The mechanisms of release of inert gases and nitrogen from nitride are different: the diffusion mechanism for inert gases and the knocking out of fission fragments for nitrogen. The difference in the gas release mechanisms leads to a significant quantitative difference in the gases release under the cladding. The specific nitrogen yield under the fuel pin cladding is significantly lower than the specific yield of other gases, but its presence is an important factor, since the dissociation temperature of the mixed nitride, as well as the nitriding of the inner surface of the cladding, depends on the nitrogen pressure under the fuel pin cladding. A generalization and analysis of the results of post-irradiation examinations of the nitrogen content in the gas mixture under the claddings of 87 investigated fuel pins after irradiation in the BN-600 reactor as part of 17 experimental fuel assemblies with mixed uranium-plutonium nitride fuel, irradiated to maximum fuel burn-up from 3 at. % to 9 at. % is carried out in the paper.
Examinations of fuel elements with two different fuel compositions, U-Mo+Mg and UO2+Mg, irradiated in the AM reactor after their long-term storage do not reveal any visible defects on the surface of their outer claddings. However, in the fuel elements with U-Mo fuel, an increase in the diameter of the outer cladding is observed. This is most noticeable in the upper part of the fuel element. Storage of the fuel elements with UO2 fuel for 15–22 years does not lead to a change in their diameter within the measurement accuracy. At the same time, metallographic studies have shown that on the external surface of the outer cladding and the internal surface of the inner cladding of the fuel elements with U-Mo+Mg and UO2+Mg fuel compositions, after long-term storage, defects are observed in the form of intergranular and irregular frontal corrosion, pits and pittings up to 20 µm deep. No interaction is found at the points of contact between the fuel claddings and the fuel composition of the layers. There is no noticeable decrease in the thickness of the outer and inner claddings of the fuel elements after long-term storage, nor does the thickness of the claddings at the locations of defects go beyond its minimum initial value, taking into account the technological tolerance for variations in thickness. It is noteworthy, however, that cracks are found in both types of fuel elements both in the fuel grains and in the magnesium matrix. As a result of long-term storage of the fuel elements with U-Mo fuel for 45–55 years, the mechanical properties of their outer claddings gradually degrade, due to which the plasticity of the cladding is significantly reduced.