1 August 2019 in IOP Conference Series: Materials Science and Engineering
This study explores how 0.23% tantalum and 0.47% niobium in tin slag from the Bangka-Belitung archipelago, Indonesia, are upgraded. To enrich the contents of both metals, this research involves 8M NaOH leaching followed by 0.5M, 1M, and 1.5M phosphoric acid. First, tin slag was roasted at 900°C for 2 hours. Then, the sample was NaOH-leached while H3PO4 was exploited to leach its residues. Next, each of the residues from the leaching processes was characterized by XRF while the filtrates characterization used AAS and ICP-OES. On the one hand, NaOH leaching has proven to decrease the contents of iron, calcium, titanium, and aluminum. On the other hand, 0.5 M H3PO4 leaching optimizes tantalum contents up to 0.85% while 1.0 M H3PO4 leaching maximizes niobium contents up to 1.45%.
1 August 2019 in IOP Conference Series: Materials Science and Engineering
Indonesia is rich in tin ores. Slags from processing of tin ores naturally contain substantial amount of valuable metals, in this case tiobium and tantalum. This research explores how niobium and tantalum contents in local Bangka tin slag can be enhanced using NaOH and HClO4leaching reagents. First, Bangka tin slag was NaOH-leached and, then, the slag underwent HClO4leaching. Before undergoing any processes, the contents of niobium and tantalum in Bangka tin slag were 0.47% and 0.23%, respectively. After passing two leaching processes, niobium and tantalum contents reached 1.28% and 0.79%, respectively.
1 January 2024 in AIP Conference Proceedings
The demand for affordable solar cells has encouraged the development of thin-film solar cell (TFSC) technology, which employs low-cost, readily-available, and n
1 November 2019 in IOP Conference Series: Materials Science and Engineering
Kesterite Cu2ZnSnS4 (CZTS) thin film was successfully obtained using simple dip coating Synthesis of CZTS consist of mixing copper chloride, zinc chloride, tin chloride, and thiourea into a mixture of ethanol and ethanolamine to make CZTS suspension. Soda lime glass was used as a different substrate for dip coating method. Dip coating method uses 3 cycles of dip and drying at 170°C to remove ethanol and ethanolamine and then the sample was annealed at 550°C in argon atmosphere. X-ray diffraction was used to check the formation of kesterite before and after annealing. After annealing the diffraction pattern shown high crystallinity of kesterite with little secondary phase. Using Scherrer equation we can predict the crystallite size of CZTS before and after annealing. The scanning electron microscope was used to show the morphology of the CZTS before and after annealing. It is shown that although the grain was distributed homogenously a void can be seen throughout the surface. Optical properties of samples were checked before and after annealing using UV-vis Spectrometer. The result shows that dip coating method could create a good properties CZTS.