A number of technological applications of metal organic frameworks (MOFs) require the formation of their thin films on insulator and/or conductor substrates at selected areas with desired thicknesses. However, fabrication of such MOF films often requires multi-step processes and/or sophisticated instruments. Herein, we discuss electrochemistry-induced MOF deposition, which permits the direct formation of a thin MOF film with controlled thickness at a desired area on various substrates. So far, we have reported the applicability of this deposition method for the formation of zeolitic imidazolate framework-8 (ZIF-8) films. In this method, a ZIF-8 film is formed on an insulator or conductor substrate upon applying a cathodic potential to a working electrode that is placed above the substrate. Importantly, the film is formed just below the cathodic working electrode, indicating that the position and lateral dimensions (in the mm- to µm-scale) of the film can be controlled by those of the working electrode. In addition, film thickness is controllable in the range of tens to hundreds of nanometers by adjusting potential application conditions at the cathodic working electrode. These results show that the electrochemistry-induced deposition method will provide a simple means for the fabrication of a patterned MOF film on various substrates without additional lithographic processes.
The structural integrity of atomically thin two-dimensional molybdenum disulfide (MoS 2 ) is crucial for high-temperature applications, including nanoelectronics and optoelectronics. This study explores the structural stability and electrical performance, under extended thermal exposure in air, of MoS 2 flakes synthesized via chemical vapor deposition (CVD) and mechanical exfoliation. The MoS 2 flakes, both CVD-grown and mechanically exfoliated, were subjected to heating at 200 °C with a relative humidity of 60(±5)% for a prolonged period and investigated with atomic force microscopy and Raman spectroscopy. This study shows that CVD-grown flakes developed noticeable cracks after prolonged heating, whereas mechanically exfoliated flakes mostly retained their structural integrity. Also, both types of flakes showed a decrease in layer thickness and lateral size over time, with mechanically exfoliated flakes exhibiting a comparatively smaller reduction in substrate coverage area. In addition, MoS 2 -based two-terminal devices were subjected to heating at 150 °C for approximately 1100 h, and their electrical characterization revealed a steady rise in current during constant voltage (5 V) conditions. This study enhances our understanding of MoS 2 stability and provides guidance for improving the reliability of MoS 2 -based devices in high-temperature electronic applications.