Direct selective transformation of greenhouse methane (CH4) to liquid oxygenates (methanol) can substitute energy‐intensive two‐step (reforming/Fischer–Tropsch) synthesis while creating environmental benefits. The development of inexpensive, selective, and robust catalysts that enable room temperature conversion will decide the future of this technology. Single‐atom catalysts (SACs) with isolated active centers embedded in support have displayed significant promises in catalysis to drive challenging reactions. Herein, high‐density Ni single atoms are developed and stabilized on carbon nitride (NiCN) via thermal condensation of preorganized Ni‐coordinated melem units. The physicochemical characterization of NiCN with various analytical techniques including HAADF‐STEM and X‐ray absorption fine structure (XAFS) validate the successful formation of Ni single atoms coordinated to the heptazine‐constituted CN network. The presence of uniform catalytic sites improved visible absorption and carrier separation in densely populated NiCN SAC resulting in 100% selective photoconversion of (CH4) to methanol using H2O2 as an oxidant. The superior catalytic activity can be attributed to the generation of high oxidation (NiIII═O) sites and selective C─H bond cleavage to generate •CH3 radicals on Ni centers, which can combine with •OH radicals to generate CH3OH.
Two series of ZnFe2O4 mixed cubic spinel nanoparticles were prepared by a coprecipitation method, where a solution of Fe3+ and Zn2+ was alkalised by a solution of NaOH. While the first series was prepared by a careful mixing of the two solutions, the microwave radiation was used to enhance the reaction in the other series of samples. The effect of the microwave heating on the properties of the prepared particles is investigated. X-ray powder diffraction (XRD), 57Fe Mössbauer spectroscopy and magnetometry were employed to prove the cubic structure and superparamagnetic behavior of the samples. The particle size in the range of nanometers was investigated by a transmission electron microscopy (TEM), and the N2 adsorption measurements were used to determine the BET area of the samples. The stoichiometry and the chemical purity were proven by energy dispersive spectroscopy (EDS). Additionally, the inversion factor was determined using the low temperature Mössbauer spectra in the external magnetic field. The microwave heating had a significant effect on the mean coherent length. On the other hand, it had a lesser influence on the size and BET surface area of the prepared nanoparticles.
Intracellular confinement suppresses the dynamic magnetic losses of nanoparticles after uptake, limiting their efficacy under alternating magnetic fields (AMF). A crystalline metal-organic framework (MOF) shell limits this collapse by enforcing a minimum interparticle spacing that restricts the dipolar coupling imposed by endosomal packing. A conformal UiO-66 shell about 9 nm thick grows directly on poly(ethylene glycol) (PEG)-silane-stabilized Fe3O4 nanocubes at room temperature without N,N- dimethylformamide, giving single-core nanocomposites. AC hysteresis measurements in A549 lung cancer cells show that internalization collapses the loop of PEG-coated nanocubes, which retain only 12% of their aqueous specific loss power (SLP) and 28% of their remanence ratio Mr/Mmax, whereas the MOF-shelled counterparts retain 40% and 47%. Recovering the nanoparticles from the lysed cells reopens the collapsed loops and restores Mr/Mmax to 81% and 89% of the aqueous reference, placing the origin of the loss in the spacing between cores rather than in their degradation. Under safety- compliant AMF, cells containing the nanocomposites lose metabolic activity, reaching 38% of the untreated control by day 7 despite a bulk temperature rise of 1 °C, a response absent in PEG-coated 2 particles at a matched intracellular iron load. Interparticle spacing therefore emerges as a design parameter for intracellular magnetic energy dissipation.