A study is reported on Langmuir and Langmuir-Blodgett (LB) films obtained by adding different percentages of stearic acid (SA) to poly(3-octylhiophene) (P3OT). Surface pressure-mean molecular area (pi-A) isotherms, ultraviolet-visible (UV-Vis) absorption spectrum, atomic force microscope (AFM) and dc electrical measurements have been used for characterization. From p-A isotherms, the area per monomer for condensed films (of SA) increased according to P3OT amount. Good transfer ratios were obtained for LB deposition from P3OT/SA films with higher percentage of SA. LB films revealed linear growth as monitored by UV-Vis absorption spectra. Electrical characterization showed higher conductivity for LB film with 54 wt.% of SA. AFM images of the same film revealed high roughness and presence of large size agglomerates. Finally, interdigitated electrodes (IDE) coated with P3OT/SA LB films showed to be sensitive to the presence of volatile organic compounds
In this paper, devices fabricated with a diode-like structure (electrode/polymer/electrode) from spin-coated and nanostructured (Langmuir-Schaefer) films of polythiophene derivatives were characterized by impedance spectroscopy and studied by theoretical fitting to reach a better understanding of the physical processes in the devices. The materials used for this research were the polyalkylthiophene (P3AT) derivatives poly(3-butylthiophene) (P3BT), poly(3-hexylthiophene) (P3HT), poly(3-octylthiophene) (P3OT) and poly(3-decylthiophene) (P3DT). Electrical measurements were performed from 1 Hz to 1 MHz (100 mV ac) while increasing the dc bias in the range from 0 to 2.5 V. The fittings of the experimental results were performed using equivalent circuits. By plotting the theoretical and experimental spectra on a single graph, it was possible to obtain information related to the film morphology, interfacial effects, resistance, capacitance and conductivity of the polymer, thereby enhancing the understanding of this particular type of device. Among the P3AT films, those grown by the Langmuir-Schaefer technique showed higher electrical conductivity, with the only exception being that of P3BT.