The clinical effect of bone morphogenetic protein 2 (BMP-2) delivered with an osteoplastic material depends on its time-dependent local concentration. A pronounced initial release may increase protein loss from the implantation site and the risk of dose-related adverse effects, whereas excessive retention may reduce the availability of the growth factor to cells. The release profile is therefore a major criterion for carrier selection. Aim: To compare the release kinetics of recombinant BMP-2 from commercial osteoplastic materials differing in origin, composition, and particle size. Materials and methods. Fifty-milligram samples of Regegraft, Bio-Oss, Maxresorb, and BoneCeramic were loaded with 1.25 μg BMP-2 for 10 min at room temperature. One milliliter of 1% bovine serum albumin in 0.9% NaCl containing 0.2% NaN3 was then added. The medium was completely replaced at 0, 1, 3, 5, 24, 48, 144, 336, 504, and 672 h. Immunoreactive BMP-2 was measured using a solid-phase sandwich enzyme-linked immunosorbent assay with indirect detection (ELISA); three independent samples were tested per material. Results. At 0 h, 60.5% of BMP-2 was recovered from Regegraft, 30.7% from Bio-Oss, 7.6% from Maxresorb, and 61.4% from BoneCeramic. At 28 days, cumulative immunoreactive protein recovery reached 72.5±4.5%, 40.4±3.3%, 22.2±0.9%, and 68.9±5.7%, respectively. Detectable release from Regegraft persisted throughout 28 days. Individual medium fractions were below the assay quantification limit after 48 h for Bio-Oss and Maxresorb and from day 21 for BoneCeramic. Conclusion. The materials generated distinct profiles of initial retention and subsequent BMP-2 release. Maxresorb provided the greatest initial retention; Bio-Oss combined a moderate initial release with high residual fixation; Regegraft showed a pronounced initial release but the most prolonged subsequent protein recovery; and BoneCeramic showed a high initial release followed by an early plateau. The different behavior of Maxresorb and BoneCeramic despite an identical hydroxyapatite/β-tricalcium phosphate ratio cannot be attributed solely to particle size or nominal phase composition.