24 October 2024 in PLOS ONE
Objective: Human umbilical cord mesenchymal stem cells (hUCMSCs) hold significant promise across various clinical applications. Therefore, regulatory requirements necessitate a thorough investigation of the hUCMSCs safety before clinical trials and potential allergic reactions after transplantation. Methods: Abnormal toxicity test employed mice and guinea pigs dosed daily at 0.5×106 cells and 5×106 cells, respectively for 7 days. Acute toxicity test employed low, medium, and high doses of hUCMSCs injected into mice once, followed by observations for 23 days. In systemic allergy test, guinea pigs received low and high dose of hUCMSCs, with sensitization and excitation stages at day 14 and 21, respectively. Results: The abnormal toxicity test of hUCMSC injections revealed no abnormal reactions over a seven-day observation period, indicating the safety of this administration route. In acute toxicity studies, the high-dose hUCMSCs group resulted in fatalities due to pulmonary embolism. Conversely, the low-dose group exhibited no toxic reactions or deaths. The maximum tolerated dose was determined to be >2×107 cells/kg. Systemic active allergy test showed that high doses of hUCMSC intravenous injections did not induce allergic reactions. Conclusion: This research affirms hUCMSC injections meet safety standards for clinical cell therapy, emphasizing their safe and promising clinical utility.
1 July 2024 in International Journal of Nanomedicine
Objective: Collagen, a widely used natural biomaterial polymer in skin tissue engineering, can be innovatively processed into nanocollagen through cryogenic milling to potentially enhance skin tissue healing. Although various methods for fabricating nanocollagen have been documented, there is no existing study on the fabrication of nanocollagen via cryogenic milling, specifically employing graphene oxide as separators to prevent agglomeration. Methods: In this study, three research groups were created using cryogenic milling: pure nanocollagen (Pure NC), nanocollagen with 0.005% graphene oxide (NC + 0.005% GO), and nanocollagen with 0.01% graphene oxide (NC+0.01% GO). Characterization analyses included transmission electron microscopy (TEM), scanning electron microscopy (SEM), Fourier transform infrared (FTIR) spectroscopy, x-ray diffraction (XRD), zeta potential (ZP), and polydispersity index (PDI). Results: TEM and SEM analysis revealed that nanocollagen groups alone exhibited particle sizes of less than 100 nm. FTIR spectroscopic investigations indicated the presence of amide A, B, and I, II, and III (1800 to 800 cm− 1) in all nanocollagen study groups, with the characteristic C-O-C stretching suggesting the incorporation of graphene oxide (GO). XRD data exhibited broadening of the major peak as the proportion of GO increased from pure NC to the nanocollagen groups with GO. Zeta potential measurements indicated electrostatic attraction of the samples to negatively charged surfaces, accompanied by sample instability. PDI results depicted size diameters ranging from 800 to 1800 nm, indicating strong polydispersity with multiple size populations. Conclusion: This research demonstrated that collagen can be successfully fabricated into nanoparticles with sizes smaller than 100 nm.