15 October 2002 in Journal of Applied Physics
Silicon-rich silicon oxide thin films have been prepared by thermal evaporation of silicon monoxide in vacuum. The SiOx film composition (1.1⩽ x ⩽1.7) has been controlled by varying the deposition rate and residual pressure in the chamber. Long time stability of all films has been ensured by a postdeposition annealing at 523 K for 30 min in Ar atmosphere. Some films were further annealed at 973 K and some others at 1303 K. Raman scattering measurements have implied the formation of amorphous silicon nanoparticles in films annealed at 973 K and Si nanocrystals in films annealed at 1303 K. The latter conclusion is strongly supported by high resolution electron microscopy studies which show a high density of Si nanocrystals in these films. Photoluminescence has been observed from both amorphous and crystalline nanoparticles and interpreted in terms of band-to-band recombination in the nanoparticles having average size greater than 2.5 nm and carrier recombination through defect states in smaller nanoparticles.
1 July 2009 in Acta Physica Polonica A
1 September 1999 in Journal of Luminescence
15 September 1998 in Physical Review B
Raman scattering, photoluminescence, and x-ray diffraction measurements have been carried out in multilayers with varying CdSe sublayer thickness (2.5, 3.5, 4.0, 5.0, and 10.0 nm). The x-ray data have revealed that after annealing at 673 K in air, CdSe wurtzite type nanocrystals are formed having an average size smaller than the CdSe sublayer thickness. A strong increase in the intensity of 1 LO phonon Raman band of CdSe at room temperature has been observed for samples with 3.5 and 4.0 nm when excited by the 647.1 nm laser line. This increase is attributed to resonant conditions for Raman scattering brought about by an increase of the optical band-gap energy of CdSe layers with decreasing sublayer thickness. It is argued that this increase is not an internal strain-related, but a quantum-size effect manifested by one-dimensional carrier confinement. Assuming such a confinement and taking into consideration electrical and optical measurements, a band diagram is produced for the system, from which the values for each multilayer material is calculated. It is found that the calculated values corresponding to and 4.0 nm differ by 59 and 19 meV, respectively, from the quantum energy of the 647.1 nm (1.916 eV) laser line, thus supporting the above arguments and the idea that these structures constitute multiquantum wells. Two photoluminescence bands of CdSe layers have been observed in all multilayers. The peak of the main band shifts from 1.76 to 1.95 eV for multilayers with from 10 to 2.5 nm. This shift provides further evidence that the increase with decreasing is due to quantum-size effect.
10 January 2000 in Journal of Physics: Condensed Matter
Superlattices of a-SiOx /nc-CdSe and thin composite films of SiOx doped with CdSe nanocrystals have been investigated. The CdSe nanocrystals size in both kinds of samples was determined by x-ray diffraction and HREM measurements. A significant difference has been found in the size values determined by both methods, which has been ascribed to appreciable nanocrystal lattice deformations. Subband absorption, room-temperature photoluminescence and thermally stimulated currents have been measured. It has been observed that in the superlattices the absorption in the tail region increases as sublayer thickness decreases. A new photoluminescence band has also appeared in the superlattices having thinnest (2.5 nm) CdSe sublayers. Two new maximums at about 220 K and 240 K, not existing in the CdSe single layers studied, have been found in thermally stimulated current spectra of the composite films. Both maximums are less expressed in the superlattices. The described results have been connected with a size-induced increase in the concentration of interface defect states in CdSe nanocrystals. It has been estimated that these defects are disposed at about 0.35 eV above the highest occupied molecular orbit in CdSe.