In this work, two series of chemically reactive polymers, silane coupling agents (SCAs) and water-soluble polymers, were specifically designed as an additive to improve the ductility of slag geopolymer paste by vibration pressure technique. The influences of organic polymers on the fluidity, rheological behavior, mechanical property, porosity, and toughening mechanism of slag geopolymer were investigated. The polycondensation and bonding characteristics of organic–inorganic products were calculated by 1H liquid nuclear magnetic resonance (NMR) technology and Fourier transform infrared (FT-IR). The polymerization degree of composite geopolymer was evaluated by 29Si NMR and X-ray photoelectron spectroscopy (XPS). The microscopic morphology of the geopolymer matrix was analyzed using scanning electron microscopy (SEM). The results showed that the dosage of the KH570 and PAA-Na with 5 wt% behaved best in improving the flexural strength and the compressive strength of geopolymer in their corresponding organic series, respectively. The addition of polymers decreased the fluidity and the fluidity loss ratio of geopolymer slurry but reduced the harmful pores of hardened geopolymer. The organic polymers acting as bridge-fixed water molecules weakened the repulsion force, and formed a three-dimensional network through molecular interweaving in a geopolymer matrix. Methacryloxy in silane coupling agents and carboxyl group in water-soluble polymers may contribute to the improvement of hydration product structure through strong bonding with C-A-S-H. Microscopic measurements indicated that the addition of KH570 and PAA-Na in geopolymer could form 73.55% and 72.48% Si-O-Si with C-A-S-H gel, higher than the reference, and increase the polycondensation degree of C-A-S-H phase, reflected by the increased generation of Q2 and Q2(1Al) and the longer chain length, leading to a higher densified geopolymer matrix with high ductility.
A series of organic–inorganic composite geopolymer paste samples were prepared with slag-based geopolymer and three types of hydrophilic organic polymers, i.e., PVA, PAA, and CPAM, by ordinary molding and pressure-mixing processes. The reaction mechanism between slag-based geopolymer and organic polymers was studied by FT-IR, NMR, and SEM techniques. The experimental results showed that the slag-based geopolymer with the addition of 3% PVA presented the highest 28-day flexural strength of 19.0 MPa by means of a pressure-mixing process and drying curing conditions (80 °C, 24 h) compared with the geopolymers incorporating PAA and CPAM. A more homogeneous dispersion morphology was also observed by BSE and SEM for the 3% PVA-incorporated slag-based geopolymer. The FT-IR testing results confirmed the formation of a C–O–Si (Al) bond between PVA and the slag-based geopolymer. The deconvolution of the Q3 and Q2(1Al) species obtained by 29Si NMR testing manifested the addition of PVA and increased the length of the silicon backbone chain in the geopolymer. These findings confirmed that a composite geopolymer with high toughness can be produced based on the interpenetrating network structure formed between organic polymers and inorganic geopolymer.