Owing to its high theoretical capacity of ~4200 mAh g−1 and low electrode potential (<0.35 V vs. Li+/Li), utilising silicon as anode material can boost the energy density of rechargeable lithium batteries. Nevertheless, the volume change (~300%) in silicon during lithiation/delithiation makes stable cycling challenging. Since some of the capacity fading mechanisms do not function in solid electrolytes, silicon anodes exhibit better cycling performance in solid electrolytes than liquids. Nonetheless, capacity can fade rapidly because of the difficulties in maintaining mechanical integrity in thick/bulky electrodes, especially when high active material loading is employed to deliver practically useful areal capacity. By contrast, silicon nanostructures can relieve deformation-induced stress and enhance cycling performance. Here we report enhanced cycling performances achieved using nanostructured silicon films and inorganic solid electrolyte and show that amorphous porous silicon films maintain high capacity upon cycling (2962 mAh g−1 and 2.19 mAh cm−2 after 100 cycles).
We report propagation of exciton polaritons (EPs) in photoexcited nanofibers of thiacyanine dye over a few hundred micrometers at room temperature. We determine the complex refractive index along the nanofibers by fluorescence microscopy measurements on single nanofibers and observe its anomalous behavior due to the EP effect. The longitudinal-transverse splitting energy ($\Delta${}EL-T) is evaluated to be $\sim${}1\,\,eV. The large $\Delta${}EL-T and waveguide function of the nanofibers allow a millimeter propagation of EPs at room temperature, which is hardly realized in other systems.
Mean free path of inelastic electron scattering has been measured with a transmission electron microscope for the majority of stable elemental solids and their oxides. An oscillating behavior vs atomic number has been revealed, such that within one row of the Periodic Table, the minimum (maximum) of is observed for elements with completed (empty) outer shells. A significantly weaker dependence is observed for the oxides. The variation is ascribed to the three major factors: atomic density, number of “free” electrons per atom, and contribution of atomic core-loss transitions.
High-resolution transmission electron microscopy images of room-temperature fluid xenon in small faceted cavities in aluminum reveal the presence of three well-defined layers within the fluid at each facet. Such interfacial layering of simple liquids has been theoretically predicted, but observational evidence has been ambiguous. Molecular dynamics simulations indicate that the density variation induced by the layering will cause xenon, confined to an approximately cubic cavity of volume ≈ 8 cubic nanometers, to condense into the body-centered cubic phase, differing from the face-centered cubic phase of both bulk solid xenon and solid xenon confined in somewhat larger (≥20 cubic nanometer) tetradecahedral cavities in face-centered cubic metals. Layering at the liquid-solid interface plays an important role in determining physical properties as diverse as the rheological behavior of two-dimensionally confined liquids and the dynamics of crystal growth.