P-type nanocrystalline Bi0.4Sb1.6Te3 thick films were directly deposited on copper substrates by aerosol deposition (AD) involving shock compaction of the starting powder at room temperature. The film deposition rate was over 700 μm/min. The relative density of the films was above 95%. Films with a thickness of over 2 mm were obtained. They consisted of nanocrystals with grain sizes of several tens of nanometers. The crystal structure of the films was the same as the bulk materials prepared by spark plasma sintering (SPS) using the same starting powder. We measured the electrical conductivity, carrier concentration, Hall mobility, and thermal conductivity of the films and compared them with those of the bulk materials. The thermal conductivity of the AD film was 20-30% lower than that of the bulk materials, which is attributed to the increased number of grain boundaries and some defects in the AD films.
Aerosol deposition (AD) is a ceramic coating process that enables films to be fabricated by microparticle impact at room temperature. The optical emission during AD reported in previous studies is thought to be fracto-emission or triboemission; however, the mechanism has never been investigated in detail. In this study, the optical emission of the electric discharge generated during aerosol deposition of alumina films using He, Ar, and N2 was measured by optical emission spectroscopy. Each spectrum had peaks corresponding to the emission peaks of the carrier gas and no blackbody radiation characteristics were observed. The emission intensity was proportional to the flux of the kinetic energy of the aerosol particles, which suggested that the emission occurred via fracto-emission during particle impact. The gas temperature remained low at around 300 K, which quantitatively confirmed that AD is a room-temperature process. Graphical abstract
1 April 2007 in Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
The validity of the mechanochemical solid-state reaction by dry ball milling for synthesizing Pb(Zr, Ti)O 3 (PZT) fine ceramic powder at room temperature (RT) was evaluated using synchrotron radiation X-ray diffraction (SXRD). A mixture of PbZrO 3 (PZ) and PbTiO 3 (PT) powders with a molar ratio of 1:1 was prepared as the starting powder. To confirm the synthesis of PZT, the structural characteristics of the ball-milled samples with different milling times were investigated by analyzing the SXRD data using the Rietveld method. The solid-state reaction was nearly complete in a short milling time of 4 h at RT. After ball milling for approximately 8 h, only a single phase of PZT was detected. The Rietveld refinement for the crystal structure analysis demonstrated that slightly Ti-rich PZT, Pb(Zr 0.485(1) Ti 0.515(1) )O 3 , with a tetragonal crystal system, is synthesized in the 8 h sample. The tetragonality is sufficiently suppressed to resemble a cubic system even at RT, whereas the phase transition temperature ( TC ) is significantly high. We quantitatively demonstrate that PZT with a higher TC can be synthesized at RT by dry ball milling, despite the smaller spontaneous lattice distortion.