In powder bed fusion of metal with laser beam (PBF-LB/M), repetitive melting and solidification of newly added layers lead to thermal stresses and distortions during part build-up. Particularly at critical component features such as unsupported overhangs, super-elevated edges pose a risk in terms of crashes with the recoating system during powder spreading. Damaged recoater lips lead to irregularities in the form of stripes in the powder bed. These local inhomogeneities cause lack-of-fusion porosity and geometric defects on the part surface. However, quantitative information on important quality aspects, such as tensile properties, dimensional accuracy, roughness, and hardness of parts printed under irregular powder bed conditions is scarce. Here, we show that samples from build jobs with recoater crashes maintain their elastic tensile properties and hardness, but lose elongation at break. Finite-element simulations of in-process distortions are used to design an artifact that intentionally damages the silicone rubber lip of the recoater but does not cause machine breakdown. The lowest mean yield strength of the damage-affected samples is 243 MPa, which is still within the material data sheet limits for AlSi10Mg. Therefore, recoater crashes do not necessarily result in rejects, but users must consider the likely presence of porosity.
10 September 2024 in Fatigue & Fracture of Engineering Materials & Structures
Laser‐based powder bed fusion (PBF‐LB) has gained prominence in the realm of additive manufacturing of metals. This technique utilizes a laser beam to consolidate powder layers, which inherently introduces high thermal gradients and rapid cooling rates. This results in characteristic process effects, including inhomogeneities, surface roughness, anisotropy, and residual stress, which play a pivotal role in altering the fatigue properties of the manufactured components. This paper presents fatigue tests involving samples of AlSi10Mg manufactured using PBF‐LB with varying surface roughness and residual stress. An approach to predict fatigue life based on stress amplitude, residual stress, and crack size is presented, using a smooth sample as a reference. An empirical model for fatigue life prediction is developed from experimentally measured values of fatigue life, peak surface roughness, and residual stress.
5 February 2025 in Progress in Additive Manufacturing
Laser-based powder bed fusion (PBF-LB) is an advanced additive manufacturing technique renowned for its precision and capability to fabricate complex metal components. However, the high thermal gradients and rapid cooling rates intrinsic to this process introduce significant process-induced effects, such as inhomogeneities, surface roughness, anisotropy, and residual stress, all of which critically influence the fatigue behavior of the produced parts. This study investigates the fatigue performance of AlSi10Mg samples produced by PBF-LB, examining the impact of varying surface conditions, geometries, and residual stress levels. Fatigue-life prediction models are formulated based on nominal stress amplitude, residual stress, form factor, crack-initiating inhomogeneity, and surface roughness, with smooth samples serving as a baseline reference. The study presents two empirical models for predicting fatigue life and fatigue strength using S–N curves and the Kitagawa–Takahashi diagram with the El Haddad approach, derived from comprehensive experimental data, including finite element modeling, fatigue-life measurements, surface roughness evaluations, and residual stress analysis.
1 October 2023 in HTM Journal of Heat Treatment and Materials
Laser-based powder bed fusion of metals exhibit process-induced anisotropy and residual stresses, making post-manufacturing heat treatment occasionally beneficial. For AlSi10Mg, a T6 heat treatment (solution annealing, quenching, artificial aging) is recommended. Nevertheless, mechanical strength decreases as (1) the eutectic Si network dissolves, (2) the amount of dissolved Si in the Al grains decreases, and (3) the size of the silicon particles and aluminum crystals increases during solution annealing. This changes the mechanical characteristics directly or by influencing the formation of precipitation during the aging process. The success of solution annealing is affected by the annealing duration and the part’s temperature at the moment of quenching. Short annealing durations dissolve a sufficient amount of Si and Mg in the Al matrix. Therefore, both the annealing temperature’s holding duration and the heating process significantly impact the resulting microstructure. In this study, samples of different shape and size where subjected to a T6 heat treatment with different solution annealing temperatures and durations. The influence on mechanical properties after quenching and aging was investigated by hardness and tensile tests. Maximum strength is achieved by quenching promptly upon reaching the solution annealing temperature, while longer durations reduce strength as explained by the Larson-Miller parameter.
Osseointegration is highly desirable for implants used for bone replacement. Polyetheretherketone (PEEK) is an attractive material due to its characteristics such as high biocompatibility and Young's modulus similar to human bones. However, PEEK is bioinert, meaning cells do not adhere and proliferate on its surface. This problem is addressed in this study, with the goal of enhancing osseointegration of additively manufactured PEEK. The influences of surface modifications and porous structures on cellular behavior were assessed by wettability and in vitro tests with subclone of the human osteosarcoma cell line‐2 osteoblasts. Overall, the combination of surface modification, type of plasma process used, atmospheric pressure versus vacuum‐based, and surface structuring, especially gyroid structures, improve the cellular proliferation on PEEK. Therefore, its ability to enhance osseointegration is highly promising.