Anisa Purwitasari

Anisa Purwitasari

Auto-generated profile, based on publicly available information

Anisa Purwitasari

Institute for Pulsed Power and Microwave Technology (IHM) Karlsruhe Institute of Technology (KIT) Eggenstein‐Leopoldshafen Germany

Research Focus & Metrics

Academic Career Length

1Year (2026-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
13 October 2026 in Energy Technology
Verified
Journal Article
Open access
PDF file
MZMargaux Zehnder
Margaux Zehnder
APAnisa Purwitasari
Anisa Purwitasari
AHAnnette Heinzel
Annette Heinzel
KNKlarissa Niedermeier
Klarissa Niedermeier
Thermal‐energy‐storage (TES) systems are promising for decarbonizing industry by storing waste heat generated by high‐temperature processes. Used as heat transfer fluid (HTF), liquid‐metal‐based TES offer a broad liquid operating range and high thermal conductivity, making them especially attractive. Directly combining a solid storage material with metallic heat‐transfer fluid in a packed bed further increases stored energy while reducing the volume of liquid metal. Ceramics can be used as storage materials. However, liquid metals are highly corrosive. This study investigates the corrosion behavior of two grades of magnesium aluminate spinel (alumina‐rich spinel, fused spinel) and three grades of magnesium oxide (94%, 97%, and 99% purity) exposed to static liquid lead at 750 °C. The materials were analyzed using scanning electron microscopy and X‐ray diffraction. The results show that all samples performed well overall. MgO showed better resistance than the tested spinels, with the highest‐grade purity performing best. In all three grades, the magnesium oxide phase was stable; only the various calcium silicate phases observed at the grain boundaries reacted with Pb. Regarding the spinel, the fused one displayed cracks, and the alumina‐rich one displayed Pb penetration and thermal alteration, resulting in a transformation of Mg 0.38 Al 0.62 (Al 1.79 )O 4 , MgO 0.388 Al 2.408 O 4 , and corundum Al 2 O 3 , to ((Mg 4 Al 0.6 )Al 1.8 O 4 ).

24 September 2026 in Energy Storage
Verified
Journal Article
Open access
AHAnnette Heinzel
Annette Heinzel
APAnisa Purwitasari
Anisa Purwitasari
RFRenate Fetzer
Renate Fetzer
AWAlfons Weisenburger
Alfons Weisenburger
KNKlarissa Niedermeier
Klarissa Niedermeier
Liquid lead (Pb) is an attractive heat transfer fluid (HTF) for packed‐bed thermal energy storage (TES) systems aimed for high temperatures. However, liquid Pb is corrosive and its corrosivity increases with rising temperature. Therefore, compatibility tests of possible filler materials with Pb are mandatory. This study tested the corrosion and thermal alteration of seven ceramic materials (two alumina materials, one alumina zirconia composite material, two zirconia ceramics stabilized with either yttria or ceria, and two zirconium silicates in different compositions) in liquid Pb at 650°C and 750°C in a reducing environment for up to 5000 h. The results showed that the tested zirconium silicates are not suitable due to the high glass content and the ceria stabilized ZrO 2 revealed a poor thermal shock resistance. In contrast, the yttria stabilized ZrO 2 and the alumina zirconia composite showed a very good compatibility with a negligible reaction with Pb.