To compare the marginal gap and fracture resistance of implant-supported 3-dimensional (3D) printed definitive composite crowns with those fabricated by using 3 different millable materials. A prefabricated abutment was digitized by using a laboratory scanner (E4 Lab Scanner) and a complete-coverage maxillary first premolar crown was designed (Dental Designer). Forty crowns were fabricated either by 3D printing (Saremco Print Crowntec, SP) or milling (Brilliant Crios, BC; Vita Enamic, VE; Cerasmart 270, CS) (n = 10). Baseline marginal gap values were evaluated by measuring 60 predetermined points on an abutment (15 points for each side) with a stereomicroscope at ×40 magnification. Marginal gap values were reevaluated after adhesive cementation. Load-to-fracture test was performed by using a universal testing machine. Two-way analysis of variance (ANOVA) was used to evaluate the effect of material type and cementation on marginal gap values. While Tukey HSD tests were used to compare the materials' marginal gap values before and after cementation, the effect of cementation on marginal gap values within each material was analyzed by using paired samples t-tests. Fracture resistance data were analyzed by using 1-way ANOVA (α=0.05). Material type and cementation significantly affected marginal gap values (P < .001). Regardless of cementation, SP had the lowest marginal gap values (P < .001), while the differences among milled crowns were nonsignificant (P ≥ .14). Cementation significantly increased the marginal gap values (P < .001). Material type did not affect fracture resistance values (F = 1.589, P = .209). Implant-supported 3D-printed composite crowns showed higher marginal adaptation compared with the milled crowns before and after cementation. In addition, all crowns endured similar forces before fracture.
This study examined the surface roughness (Ra) and shear bond strength (SBS) of Yttria-stabilized tetragonal zirconia polycrystalline (Y-TZP) ceramic after airborne particle abrasion at different pressures and particle sizes, pre- and post-sintering. Ninety specimens, prepared from Y-TZP ceramic blocks (Vita In-Ceram YZ, Vita Zahnfabrik), were divided into nine subgroups: control, and 50 and 110 µm Al2O3 airborne particle abrasion at 3 and 4 bar pressure, before and after sintering, respectively. According to the sintering order, before and after surface treatments, Ra values were measured using a profilometer. SBS to Y-TZP was assessed after thermocycling, using self-adhesive resin cement (Rely X U200, 3M ESPE). Scanning electron microscopy (SEM) and X-ray diffractometry (XRD) were performed on one specimen per group. All surface-treated samples were rougher than the controls. ABS50-4 (50 µm Al2O3 airborne particle abrasion at 4 bar pressure before sintering), ABS110-3, and ABS110-4 showed the highest Ra values, among all cohorts. The controls displayed lower SBS values than the treated groups (p<0.05), which had statistically similar results to each other. Airborne particle abrasion of pre-sintered Y-TZP, followed by sintering, increased the tetragonal structure contents.
28 November 2020 in European Journal of Oral Sciences