The aim of this article is to provide a brief insight regarding the recent studies and their recommendations related to the modifications to glass ionomer cement (GIC) powder in order to improve their properties. An electronic search of publications was made from the year 2000 to 2018. The databases included in the current study were EBSCOhost, PubMed, and ScienceDirect. The inclusion criteria for the current study include publication with abstract or full-text articles, original research, reviews or systematic reviews, in vitro, and in vivo studies that were written in English language. Among these only articles published in peer-reviewed journals were included. Articles published in other languages, with no available abstract and related to other nondentistry fields, were excluded. A detailed review of the recent materials used as a filler phase in GIC powder has revealed that not all modifications produce beneficial results. Recent work has demonstrated that modification of GIC powder with nano-particles has many beneficial effects on the properties of the material. This is due to the increase in surface area and surface energy, along with better particle distribution of the nano-particle. Therefore, more focus should be given on nano-particle having greater chemical affinity for GIC matrix as well as the tooth structure that will enhance the physicochemical properties of GIC.
1 September 2017 in Materials Science and Engineering: C
Application of ZnO is widely used in many industries, such as in optoelectronic devices, automotive, textile, cosmetics, medical and dentistry. In this study, emphasis was given on ZnO-eugenol (ZOE) that has been used in dental restoration. ZOE contained 80% ZnO and 20% eugenol. ZOE exhibited selective toxicity that could kill bacteria but safe on human cells. The safety of ZOE on humans is critically important. Two types of ZnO with different morphology, namely ZnO-A and ZnO-K were used to make ZOE (ZOE-A and ZOE-K) and the cytotoxicity level on human gingival fibroblast (HGF) cell line were evaluated. Both ZnO were characterized for its morphology and structural using Field Emission Scanning Electron Microscopy (FESEM) and X-ray Diffraction (XRD), respectively. The cytotoxicity level was evaluated using CCK-8 assay where the percentage of viable cells after 72 h were observed. The result showed ZnO-A, containing mostly rod-like shape with a crystallite size of 37.5 nm, had a higher percentage of viable cells after 72 h. Sample ZnO-K, containing irregular shape morphology with bigger crystallite size of 42.2 nm, had a lower percentage of viable cells after 72 h. The HGF cell line was treated with extract dilution of ZOE-A and ZOE-K at 5, 10 and 15%, respectively. At 15% of extracts dilution, 97.3% of the HGF cells survived (for ZOE-A) while the survival percentage of ZOE-K was only 88.1%. This fact was probably due to the larger surface-to-volume ratio of ZnO-A that gave better interlocking bond in ZOE-A. This interlocking bond can prevent the ZnO and eugenol elements leaching out from the ZOE matrix thereby decrease in cytotoxicity effects on HGF.