1 February 2016 in Current Applied Physics
21 June 2019 in Physical Review B
We report the infrared transmission measurement on electrically gated twisted bilayer graphene. The optical absorption spectrum clearly manifests dramatic changes such as the splitting of the interlinear-band absorption step, the shift of the inter-van Hove singularity transition peak, and the emergence of a very strong intravalence (intraconduction) band transition. These anomalous optical behaviors demonstrate consistently a nonrigid band structure modification created by ion-gel gating through layer-dependent Coulomb screening. We propose that this screening-driven band modification is a universal phenomenon that persists to other bilayer crystals in general, establishing electrical gating as a versatile technique to engineer band structures and to create different types of optical absorptions that can be exploited in electro-optical device applications.
2 December 2016 in Physical Review B
We measured Drude absorption of gated CVD graphene using far-infrared transmission spectroscopy and determined the carrier scattering rate () as a function of the varied carrier density (). The -dependent was obtained for a series of conditions systematically changed as (10 K, vacuum) (300 K, vacuum) (300 K, ambient pressure), which reveals that (1) at low-T, charged impurity () and short-range defect () are the major scattering sources which constitute the total scattering , (2) among various kinds of phonons populated at room-, surface polar phonon of the substrate is the dominantly scattering source, and (3) in air, the gas molecules adsorbed on graphene play a dual role in carrier scattering as charged impurity center and resonant scattering center. We present the absolute scattering strengths of those individual scattering sources, which provides the complete map of scattering mechanism of CVD graphene. This scattering map allows us to find out practical measures to suppress the individual scatterings, the mobility gains accompanied by them, and finally the ultimate attainable carrier mobility for CVD graphene.
7 April 2017 in Discover Nano
We report on a thickness-dependent wetting property of WS2/Al2O3 and WS2/SiO2/Si structures. We prepared WS2 films with gradient thickness by annealing thickness-controlled WO3 films at 800 °C in sulfur atmosphere. Raman spectroscopy measurements showed step-like variation in the thickness of WS2 over substrates several centimeters in dimension. On fresh surfaces, we observed a significant change in the water contact angle depending on film thickness and substrate. Transmission electron microscopy analysis showed that differences in the surface roughness of WS2 films can account for the contrasting wetting properties between WS2/Al2O3 and WS2/SiO2/Si. The thickness dependence of water contact angle persisted for longer than 2 weeks, which demonstrates the stability of these wetting properties when exposed to air contamination.
25 February 2019 in Applied Physics Letters
We performed infrared transmission experiment on ion-gel gated graphene and measured carrier scattering rate γ as a function of carrier density n over a wide range up to n = 2 × 1013 cm−2. γ exhibits a rapid decrease along with the gating followed by a persistent increase upon further carrier doping. This behavior of γ(n) demonstrates that the carrier is scattered dominantly by the two scattering mechanisms, namely, charged impurity (CI) scattering and short-range disorder (SR) scattering, with additional minor scattering from substrate phonons (SPP). We can determine the absolute strengths of all the scattering channels by fitting the γ(n) data and unveil the complete n-dependent map of the scattering mechanisms . and are larger than those of SiO2-gated graphene by 1.8 times, which elucidates the dual role of the ion-gel layer as a CI-scatterer and simultaneously a SR-scatterer to graphene. Additionally, we show that freezing of IG at low-T (∼200 K) does not cause any change to the carrier scattering.