Two novel composite propellant formulations have previously been produced from a binder consisting of the thermoplastic elastomer styrene‐ethylene/butylene‐styrene (SEBS) and a solid filler, either ammonium perchlorate (AP) or 1,3,5‐trinitro‐1,3,5‐triazinane (RDX). The binder, being a commercially available off‐the‐shelf polymer, has many advantages over a typical bespoke binder, particularly cost and risk of obsolescence. The thermal and hazard properties have shown potential for these formulations. This paper addresses the mechanical properties over a range of service and storage temperatures, which is important in the safety and durability of a propellant. The glass transition temperatures, as determined by dynamic mechanical analysis (DMA), were found to be influenced by the type of filler and the solids loading. The lower glass transition was seen to increase slightly from −41°C for unfilled SEBS to −39°C (AP/SEB 84/16) with AP as a filler; conversely, it decreased to −45°C (RDX/SEBS 80/20) with RDX. The upper glass transition was found to have decreased from 102°C to around 91°C for all formulations tested. Use of DMA—time temperature superpositioning found that the filler influenced the frequency dependency of the mechanical behaviour. Compared to typical AP composite propellants, both the storage modulus (E’) from DMA and Young's modulus (E) from tensile testing were substantially greater. Tensile testing also showed that the strain at maximum stress (ε m ) was significantly less. However, the maximum stress (σ max ) was similar. SEBS has shown potential as a binder for a stiffer composite propellant (higher modulus).
3 June 2024 in Journal of Polymer Science
KMKhuthadzo Lourate Mutele‐Nkuna
Khuthadzo Lourate Mutele‐Nkuna
+1
Novel elastomers are made by reaction of hydroxyl‐terminated polyacrylic ester (HyTemp) with polyethylene glycol (PEG, number of ethylene glycol units 1, 3, 6, 9) based cross‐linkers. The influence of the cross‐linker length, the HyTemp/cross‐linker (w/w) ratio and the cross‐linking accelerator trifluoromethanesulfonate scandium salt (ScTFMS) on the structure and the properties of the materials are studied. The cross‐linker length has not influence on the glass transition (Tg) of the products because of the presence of the flexible PEG units that cancels out the cross‐linking effect associated to a shift to higher Tg. A two‐domain structure is seen by the presence of a dual Tg in samples cured with ScTFMS. Mathematical analysis of the modulated differential scanning calorimetry curves offers for the first time the possibility to identify/confirm structural differences in complex three‐dimensional polymeric structures. Scanning electron microscopy and swelling experiments in ethyl acetate respectively reveal an increase in the pore size (1.13 to 5.48 nm) and in the absorption ability of the elastomers cured with different types and quantities of PEG cross‐linker. The new elastomeric materials are exhibiting a rubbery state over a wide temperature range and absorptivity for the potential recovery of pollutants in soil and/or water.