Fan Mo

Fan Mo

Auto-generated profile, based on publicly available information

Fan Mo

Shanghai Key Lab for R&D and Application of Metallic Functional Materials, School of Materials Science and Engineering, Tongji University, Shanghai 201804, China

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
20 May 2019 in Metals
Verified
Journal Article
Open access
PDF file
CYCheng Yao
Cheng Yao
ZHZheng-Fei Hu
Zheng-Fei Hu
FMFan Mo
Fan Mo
YWYu Wang
Yu Wang
Aluminum Foam Sandwich panels were fabricated via liquid diffusion welding and glue adhesive methods. The Microstructure of the Aluminum Foam Sandwich joints were analyzed by Optical Microscopy, Scanning Electron Microscopy, and Energy Dispersive Spectroscopy. The metallurgical joints of Aluminum Foam Sandwich panels are compact, uniform and the chemical compositions in the diffusion transitional zone are continuous, so well metallurgy bonding between Aluminum face sheet and foam core was obtained. The joining strength of an Aluminum Foam Sandwich was evaluated by standard peel strength test and the metallurgical joint Aluminum Foam Sandwich panels had a higher peel strength. Moreover, a three-point bending fatigue test was conducted to study the flexural fatigue behavior of Aluminum Foam Sandwich panels. The metallurgical joint panels have a higher fatigue limit than the adhesive joining sandwich. Their fatigue fracture mode are completely different, the failure mode of the metallurgical joint is faced fatigue; the failure mode for the adhesive joint is debonding. Therefore, the higher joining strength leads to a longer fatigue life.

11 July 2021 in Metals
Verified
Journal Article
Open access
PDF file
ZDZexu Du
Zexu Du
ZHZheng-Fei Hu
Zheng-Fei Hu
Yuqiang FengYuqiang Feng
Yuqiang Feng
FMFan Mo
Fan Mo
Two kinds of 60NiTi powders were prepared by pure Ni mixed with Ti powders, and 55NiTi alloy powder with pure Ni powder and both the powders were fully mixed by alcohol ball milling. Two kinds of coatings (denoted as 60Ni-40Ti and 55NiTi-5Ni) were prepared on a 316L stainless steel substrate by laser cladding. The microstructure, microhardness and electrochemical behavior of the prepared coatings were investigated extensively. The results show that 55NiTi-5Ni has a typical dendritic eutectic structure, but 60Ni-40Ti tends to form a eutectic network structure. The main phases in both coatings are (Ni, Fe)Ti and (Ni, Fe)3Ti; however, the (Ni, Fe)Ti phase is dominant in 55NiTi-5Ni, but the (Ni, Fe)3Ti phase is more prevalent in 60Ni-40Ti. The microhardness was significantly improved with the 316L stainless steel substrate, and the microhardness of 55NiTi-5Ni is slightly higher than 60Ni-40Ti. The corrosion resistance of the two coatings in 3.5 wt% NaCl solution also leads to significant improvements compared with the substrate, and the corrosion resistance of 55NiTi-5Ni was also increased. These different behaviors and characteristics might be related to the different microstructures. Uniform and fine eutectic structure in 55NiTi-5Ni coating lead to better performance, which is also conducive to the formation of the dense oxide film to improve corrosion resistance.

28 September 2021 in Metals
Verified
Journal Article
Open access
PDF file
YCYao Cheng
Yao Cheng
ZHZheng-Fei Hu
Zheng-Fei Hu
FMFan Mo
Fan Mo
The monotonic and fatigue strength of adhesively bonded aluminum foam sandwich panels with different densities of core aluminum foam (0.3 g/cm3, 0.4 g/cm3, 0.6 g/cm3) were investigated in three-point bending tests to study the flexural fatigue behavior of aluminum foam sandwich panels. The force cycle curves, deflection curves, and hysteretic curves are presented to describe the fatigue process of aluminum foam sandwich panels. Their fatigue fracture modes are completely different, the failure modes of the low-density cores (0.3 g/cm3, 0.4 g/cm3) are debonding and face fatigue, whereas the failure mode of the high-density core (0.6 g/cm3) is face fatigue without debonding. The reason is that high-density aluminum foam cores with lower porosity have a larger joining face, which can also provide higher strength and lead to a longer fatigue life.

5 November 2020 in Electrochemistry
Verified
Journal Article
Closed access
MBMingcheng Bing
Mingcheng Bing
FMFan Mo
Fan Mo
ZHZheng-Fei Hu
Zheng-Fei Hu