Newly fabricated semiconductor Bi2O2Se films exhibit excellent electron transport and optical properties, with potential application in optoelectronics. In this work, using first-principle calculations combined with the modified Becke-Johnson exchange potential, we have systematically investigated the electronic, transport, and optical properties of bulk Bi2O2Se. Our calculations have shown that external strain can effectively tune the bulk Bi2O2Se electronic bandgap and optical response and that, in particular, the appropriate strain can lead to a transition from an indirect to a direct bandgap. In addition, we found that electron mobility increased with Bi2O2Se crystal thickness and that the computed bulk Bi2O2Se acoustic-phonon-limited electron mobility could reach ∼940 and 535 cm2 V−1 s−1 in the a(b) and c directions at 300 K—which was much higher than that (∼50 cm2 V−1 s−1) achieved by the monolayer. There was a clear anisotropy of the electron mobility in bulk Bi2O2Se, which could be attributed to the synergistic effect between the elastic modulus anisotropy and the deformation potential. Our results not only have given new insight into the high carrier mobility of different thickness Bi2O2Se films (monolayer to bulk) but have also revealed the importance of the electron-transport direction to device performance. Together with the high carrier mobility, strain-tunable electronic structure, and optical response, Bi2O2Se films with different thicknesses have been shown to be very attractive for application to optoelectronic and electronic devices.
1 April 2017 in Physica E: Low-dimensional Systems and Nanostructures
Forming solid solutions is one of the most effective strategies to suppress the thermal conductivity of thermoelectric materials. However, the accompanying increase in impurity ion scattering usually results in an undesirable loss in hall mobility, negatively impacting the electrical transport properties. In this work, a tellurium–selenium (Te-Se) solid solution with trace antimony (Sb) doping was synthesized via the high pressure and high temperature method. It was found that slight Se doping into the Te sites not only had no impact on the hall mobility and carrier concentration, but also enhanced the density-of-state effective mass of Sb0.003Te0.997, leading to an enhanced power factor near room temperature. Additionally, the presence of Se doping caused a significant reduction in the phonon thermal conductivity of Te due to fluctuations in the mass and strain field. The lowest phonon thermal conductivity was as low as ~0.42 Wm−1K−1 at 600 K for Sb0.003Se0.025Te0.972, which approached the theoretical minimum value of Te (~0.28 Wm−1K−1). The effects of Se doping suppressed thermal conductivity, while Sb doping enhanced the power factor, resulting in a larger ZT of ~0.94 at 600 K. Moreover, these findings demonstrate that Sb and Se doping can effectively modulate the electrical and thermal transport properties of Te in a synergistic manner, leading to a significant increase in the average ZT across a wide temperature range.