Mixtures of Ni-based filler metal without and with 0.5, 1, and 2% WC nanoparticles (NPs) were methodologically tested in order to improve the wear behaviour of WC/Ni-based overlays deposited on low carbon steel by the plasma transferred arc (PTA) process. On adding 2% WC NPs, the longitudinal direction overlay microstructure was modified to have a fibrous appearance. The mechanism to improve WC particle distribution and thus prevent microcrack propagation in the overlays implies a liquid-phase viscosity change. Results of pin-on-disk tests in the overlay using filler metal with 2% WC NPs show that the combined effect of fibrous microstructure and W-rich phases in the overlay, decreases the volume loss by 76% and 78% in comparison with overlays without WC NPs for a 1 and 5 N load, respectively. These outcomes might be of interest for the mining industry, where machinery and equipment are exposed to extreme wear conditions.
In order to improve the Mg removal from an A-380 molten alloy, mixtures of zeolite and SiO2nanoparticles () were tested. Zeolite was enriched with 2.5, 5, 7.5, 10, or 12.5 wt-% of amorphous. Theand zeolite were mixed for 30 min in ethanol for each experiment and then dried in a furnace at 80°C for 12 h. The enriched zeolites were analyzed by scanning electron microscopy, transmission electron microscopy, and N2gas adsorption analysis. The Mg removal was carried out injecting each mixture into the molten aluminum alloy at 750°C using argon. The Mg content of the molten alloy was measured after different periods of the injection time. Zeolites enriched with 2.5 and 5 wt-% ofwere demonstrated to be the better mixtures, removing Mg from an initial content of 1.6 to a final content of 0.0002 and 0.0101 wt-%, respectively, in 45 min of injection.