A. B. Baldissera

A. B. Baldissera

Auto-generated profile, based on publicly available information

A. B. Baldissera

Metals and Alloys University of Bayreuth Prof.‐Rüdiger‐Bormann‐Str. 1 95447 Bayreuth Germany

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
14 June 2017 in IEEE Transactions on Magnetics
Verified
Journal Article
Closed access
ABA. B. Baldissera
A. B. Baldissera
PPP. Pavez
P. Pavez
PWP. A. P. Wendhausen
P. A. P. Wendhausen
CAC. H. Ahrens
C. H. Ahrens
JMJ. M. Mascheroni
J. M. Mascheroni
Isotropic bonded magnets were fabricated by powder bed fusion additive manufacturing (AM) using a feedstock composed of polymeric binder polyamide 12 (PA-12) and a near stoichiometric Nd2Fe14B atomized nanocrystalline powder. The AM equipment constructed for that purpose uses a computer controlled laser beam to melt the binder and build parts layer by layer. Three process parameters were evaluated: layer thickness, hatch spacing and laser power. For the evaluation of magnetic properties, cylindrical samples with diameter and height of 10 mm were produced and measured in a hysteresisgraph. For a feedstock based on a 34 % volumetric fraction of PA- 12, the highest density value achieved was 3.6 g/cm³, resulting in a remanence of 0.3 T. These relatively low values for remanence are due to the isotropic characteristic of the powder, the binder fraction and the interparticle porosity not being completely eliminated. Results indicate that layer thickness affects densification more significantly than laser power and hatch spacing. Consequently remanence follows the same trend. Coercivity has not been affected much by optimized process parameters, since the values of original atomized powder of around 700 kA/m remained practically the same. The overall conclusion of this study shows encouraging results to explore this alternative AM technique to produce net shape permanent magnets.

1 October 2019 in Journal of Rare Earths
Verified
Journal Article
Closed access
JEJ.A.B. Engerroff
J.A.B. Engerroff
ABA.B. Baldissera
A.B. Baldissera
MMM. D. Magalhães
M. D. Magalhães
PLP.H. Lamarão
P.H. Lamarão
PWP.A.P. Wendhausen
P.A.P. Wendhausen
JMJ.M. Mascheroni
J.M. Mascheroni

21 July 2025 in Advanced Engineering Materials
Verified
Journal Article
Open access
ABAndré Baldissera
André Baldissera
SBSean Böhm
Sean Böhm
RVRainer Völkl
Rainer Völkl
UGUwe Glatzel
Uwe Glatzel
Appropriate conditions to obtain single‐crystal (SX) castings of the nickel‐based superalloy CM186LC, developed for directional solidification, are investigated. Cylindrical samples with starter blocks and grain selectors are cast via a proprietary SX Bridgman process. The effect of the solidification rates ( V ) ranging from 1 to 10 mm⋅min −1 on the microstructure is explored. Primary dendrite arm spacings ( λ p ) fall within the expected range of 200–500 μm. Single crystal is achieved at V ≅ 3 mm⋅min −1 . The growth direction of the crystals in all cases diverges strongly from [001] orientation. Different solidification behavior of CM186LC compared to otherwise chemically similar CMSX‐4 is attributed to minor additions of grain boundary strengtheners C, Hf, B, and Zr.