Rathinavelu Venkatesh

Rathinavelu Venkatesh

Auto-generated profile, based on publicly available information

Rathinavelu Venkatesh

Department of Mechanical Engineering, Saveetha School of Engineering, Saveetha Institute of Medical and Technical Sciences, SIMATS, Chennai, India

Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
16 June 2023 in Biomass Conversion and Biorefinery
Verified
Journal Article
Closed access
PDF file
RSR. Sasikumar
R. Sasikumar
SPS. Prabagaran
S. Prabagaran
RVR. Venkatesh
R. Venkatesh
SKS. Kumaravel
S. Kumaravel

1 January 2022 in Journal of Nanomaterials
Verified
Journal Article
Open access
PDF file
RVR. Venkatesh
R. Venkatesh
MSMANIVANNAN SUBRAMANIAN
MANIVANNAN SUBRAMANIAN
SKS. Kaliappan
S. Kaliappan
SSS. Socrates
S. Socrates
SSS. Sekar
S. Sekar
MBMelkamu Beyene Bayu
Melkamu Beyene Bayu
The objective of the present experimental work is to obtain an appropriate welding parameter on pulsed current gas tungsten arc welding (GTAW) ferritic stainless steel AISI 409L with a thickness of 4.5 mm. Frequency affected penetration, and the ratio of bead width to penetration (aspect ratio) is the main objective of the research. A Taguchi L9 orthogonal array with three level four factors was chosen to execute the bead on plate welding. It leads to optimize the input process parameters on main effect plot via analysis of variance, and it has imposed to determine their contribution level of each parameter with respect to responses. Taguchi optimized conditions for butts weld with the pulsed TIG and its surface morphology, and mechanical characteristics of AISI 409L weld was investigated. A full penetration with an optimal aspect ratio was accomplished using high‐frequency pulsing, according to the findings. The mechanical properties were characterized using Vickers microhardness and tensile tests on the base material and weld metals. Microstructural study revealed that these variables have a greater impact on the bead profile. Pulsed TIG showed maximum UTS of 445 MPa and a minimum of 385 MPa, with an average of three samples of 415 MPa. The weld metal in all of the zones had influenced superior tensile strength (UTS) as compared to base metal, according to the findings. The obtained strain percentage for both butt and TIG welds, however, was smaller than that of the parent metal. The formation of martensitic was attributed for the higher tensile strength with minimized ductility of the pulsed TIG welds. Furthermore, results on the hardness are in concurrence with the tensile experiments, as the zone for fusion has a higher hardness than the base metal. Corrosion behavior of the parent metal and welded specimen was analyzed using a potentio‐dynamic polarization technique. The electrochemical behavior of base material and weld samples confirmed that the overall corrosion resistance is better in parent material than the other zones.

3 May 2023 in Heliyon
Verified
Journal Article
Open access
RVR. Venkatesh
R. Venkatesh
SBSuhas Ballal
Suhas Ballal
AKA. Mohana Krishnan
A. Mohana Krishnan
SPS. Prabagaran
S. Prabagaran
MSMohankumar S
Mohankumar S
ERElangomathavan Ramaraj
Elangomathavan Ramaraj
Natural fiber-reinforced polymer matrix composites are gathering significance in future trend applications such as automotive, aerospace, sport, and other engineering applications due to their superior enhanced mechanical, wear, and thermal properties. Compared to synthetic fiber, natural fiber is low adhesive and flexural strength properties. The research aims to synthesize the epoxy hybrid composites by utilizing the silane (pH = 4) treated Kenaf (KF) and sisal fiber (SF) as layering by uni, bi, and multi-unidirectional via hand layup techniques. Thirteen composite samples have been prepared by three-layer formation adopted with different weight ratios of E/KF/SF such as 100E/0KF/0SF, 70E/30KF/0SF, 70E/0KF/30SF, 70E/20KF/10SF, and 70E/10KF/20SF respectively. The effect of layer formation on the tensile, flexural, and impact strength of composites is studied by ASTM D638, D790, and D256 standards. The unidirectional fiber layer formed (sample 5) 70E/10KF/20SF composite is found maximum tensile and flexural strength of 57.9 ± 1.2 MPa and 78.65 ± 1.8 MPa. This composite is subjected to wear studies by pin-on-disc wear apparatus configured with a hardened grey cast-iron plate under an applied load of 10, 20, 30, and 40 N at different sliding velocities of 0.1, 0.3, 0.5, and 0.7 m/s. The wear rate of the sample progressively increases with increasing load and sliding speed of the composite. The minimum wear rate of 0.012 mg/min (sample 4) is found on 7.6 N frictional force at 0.1 m/s sliding speed. Moreover, sample 4 at a high velocity of 0.7 m/s with a low load (10 N) shows a wear rate of 0.034 mg/min. The wear-worn surface is examined and found adhesive and abrasive wear on a high frictional force of 18.54 N at 0.7 m/s. The enhanced mechanical and wear behavior of sample 5 is recommended for automotive seat frame applications.

1 January 2022 in Adsorption Science & Technology
Verified
Journal Article
Open access
PDF file
RVR. Venkatesh
R. Venkatesh
PSP. Raja Sekaran
P. Raja Sekaran
KUK. Udayakumar
K. Udayakumar
DJD. Jagadeesh
D. Jagadeesh
KRK. Raju
K. Raju
MBMelkamu Beyene Bayu
Melkamu Beyene Bayu
The Ag/MgO/biochar nanostructures were fabricated using a solvent-free ball milling process as an effective adsorbent. Development of functional materials capable of completely removing organic pollutants from water and their adequate adsorption present challenges. The addition of MgO nanoparticles diffused equally on biochar surfaces in the biochar matrix, according to various characterization data. In decomposing biochar and compressing MgO, powdered metal enhanced mesopores and macropores of nanocomposites. XPS analysis indicates the potential synthesis of modified biochar nanocomposites. Adequate amounts of MgO added to biochar improved the ability of the nanocomposites to remove methylene blue (M.B.) through photosynthesis and adsorption. Photocatalytic analysis was carried out for the proposed novel composites to remove tetracycline (T.C.) subjected to different conditions. The photodegradation efficiency was found 80.26% for TC concentration, 50 ppm, H2O2 of 100 mM pH: 5-6 of Ag/MgO/biochar (0.01 g) at 25° temperature. Treatment of various organic wastewaters by metal oxide/biochar nanocomposites with strong adsorption and photocatalytic degradation capabilities is made possible by this research.