Nafion β-relaxation was studied by detailed dielectric spectroscopy measurements carried out in a wide range of both temperature and relative humidity. Cast and extruded Nafion were compared in the H+, Na+, and Cs+ forms to evaluate contributions arising from membrane morphology and ionic interactions. The experimental data indicated that β-relaxation is associated with the motion of side chains of the ionomer. The unusual shift to lower frequencies of the β-relaxation was shown to be more pronounced for samples containing high water content and at temperatures above the α-relaxation, evidencing that the electrostatic repulsions between bare sulfonic groups reduce the side chain mobility. A pronounced increase of relaxation times was observed at relative humidity >60% suggesting a change of the morphology of the ionomer, in agreement with recent descriptions of the Nafion structure by small angle X-ray scattering analyzes.
In this study, both PtSn/C electrocatalysts and composites electrolytes based on Nafion and mesoporous titania (Nafion-TiO2) were evaluated in direct ethanol fuel cell operating at 130oC. PtSn/C catalysts with different compositions were prepared by alcohol-reduction process. The electrochemical activity of these electrocatalysts was verified by cyclic voltammetry and chronoamperometry measurements. Cast Nafion-TiO2 composites were characterized by differential scanning calorimetry and ac impedance spectroscopy. The water uptake of the composites was determined by gravimetry. Membrane electrode assemblies composed by Nafion-TiO2 electrolyte and PtSn/C anode were evaluate in DEFC operating in 80-130oC temperature range. Polarization curves showed an enhanced performance (maximum power density of ~50 mW cm-2) for DEFC using combined PtSn/C (60:40) electrocatalyst and Nafion-TiO2 (10 wt%) operating at 130oC.
Nafion β-relaxation was studied by detailed dielectric spectroscopy measurements carried out over a wide range of both temperature and relative humidity. Both cast and extruded Nafion were compared in the H+, Na+, and Cs+ forms to evaluate contributions arising from membrane morphology and ionic interactions. The combined data indicated that β-relaxation is related to the motion of the polymer side chains. The shift to lower frequencies of the β-relaxation was shown to be more pronounced for samples containing high water content at temperatures above the α-relaxation, evidencing that the electrostatic repulsions between bare sulfonic groups reduce the side chain mobility. An abrupt change of relaxation time was observed at relative humidity > 60% and associated with a change of morphology of the ionomer from an inverted micellar structure to a rodlike network.