20 June 2022 in International Journal of Renewable Energy Development
Lithium batteries development are triggered so many efforts in producing electronic devices due to its excellent performance as energy storage systems. One of the appealing points solid polymer electrolytes for developing solid-state lithium batteries. In this study, Solid polymer electrolytes with crosslinked treatment (SPE-C) were prepared from carboxymethyl cellulose-lithium perchlorate (CMC-LiClO4) and citric acid (CA) as a crosslinker via solution casting method. All SPE-C membranes were assembled into lithium battery coin cells. Degree of crosslinked and degradation were measured to observe crosslink formation in SPE-C membranes and confirmed by fourier transform infrared (FTIR), whereas SPE-C in coin cells were characterized by electrochemical impedance spectroscopy (EIS) and linear sweep voltammograms (LSV). The results showed that crosslinked process is successfully obtained with C=O from ester linkage of CA vibration within COO- of CMC for the crosslinking bond formation. The crosslink effect also contributed on enhancing ionic conductivities of SPE-C in coin cells from EIS results. The highest ionic conductivity was obtained in SPE-C2 (1.24×10-7 S/cm) and electrochemically stable in 2.15 V based on LSV measurement. SPE-C2 has good dielectric behavior than the others due to the high ions mobilities for migration process from ion clusters formation, thus it would be useful for further study in obtaining the powerful solid-state lithium polymer batteries.
1 February 2019 in Journal of Physics: Conference Series
Graphene/polyaniline nanocomposite has been synthesized and applied as supercapacitor electrodes. Graphene was synthesized by oxidation of graphite followed by reduction of graphite oxide to form reduced graphene oxide then transformed into graphene by reduction with NaBH4. The graphene/polyaniline nanocomposite was prepared by in situ polymerization of aniline in graphene suspension with a variation of the composition. Characterization of samples was conducted using FTIR spectrometer, XRD, and SEM. Specific capacitance was obtained from the cyclic voltammogram (CV) curve taken using the potentiostat/galvanostat. FTIR spectra shows the presence of functional groups indicating the formation of a graphene/polyaniline composite. Results of XRD analysis indicated the presence of crystal phases of graphene and polyaniline. Morphology of graphene is looked like a rather thick sheet while graphene/polyaniline nanocomposites are looked like clumps which are an incorporation of graphene and polyaniline nanoparticles. The highest specific capacitance of the supercapacitor fabricated with graphene/polyaniline electrode was 128 F/g.
10 July 2023 in TIME in Physics
Ultrasonic wave has been utilized to synthesize the ZnO nanoparticle. ZnO is formed from a mixture of zinc acetate (ZnAc) and Natrium Hydroxide (NaOH) with various concentrations of ZnAc 0.5 M (ZnO 1:1) and 1.5 M (ZnO 3:1) and the concentration of NaOH remained at a concentration of 0.5 M. The Structure and crystal size were characterized using X-ray Diffraction (XRD), while its morphology was examined by Scanning Electron Microscopy (SEM). The results show that ZnO 1:1 has a higher (stronger) diffraction intensity than the ZnO 3:1. The crystallite size of ZnO 1:1 averaged 30.57 ± 4.31 nm while the ZnO 3:1 had an average crystallite size of 20.25 ± 7.12 nm. From the size of the crystallites ZnO particles that are formed include nanoparticles. ZnO 1:1 SEM image shows the shape of microrods in the 1:1 ZnO sample while in the 3:1 ZnO sample no microrods are formed. Based on the morphology, the 1:1 ZnO sample has an average size of 230 nm and is larger than the 3:1 ZnO sample which has an average size of 50 nm.