13 September 2023 in Energy & Environmental Science
The optimal design of liquid electrolytes is vital for the build-up of long-lifespan lithium-metal batteries (LMBs) that function over a wide-temperature-range. Tuning the electrolyte solvation-structure using partially-fluorinated ether solvents and constructing stable electrode–electrolyte interfaces using electrolyte additives enhance the electrochemical reversibility of lithium-metal anodes and facilitate the realization of high-capacity cathodes for LMBs. This study reports a partially and weakly solvating electrolyte (PWSE) which enables the stable cycling of LMBs at high-voltages within a wide-temperature range through modulation of an electrolyte local-environment using a low-salt concentration of 1.3 M. 1,2-Bis(1,1,2,2-tetrafluoroethoxy)ethane contains two oxygen atoms that coordinate weakly with Li+-ions; it transforms the 1,2-dimethoxyethane-dominated electrolyte solvation-structure to a more anion-incorporated structure. Moreover, a combination of lithium fluoromalonato(difluoro)borate and silver nitrate strengthens the electrode–electrolyte interfaces and improves the oxidation durability of ether-based electrolytes. The PWSE enables the construction of 4.4 V Li|LiCoO2 full cells with a long-lifespan and high-areal-capacity of 3.12 mA h cm−2.
5 July 2024 in Energy & Environmental Science
Anode-free lithium (Li) batteries that function via direct Li plating/stripping on metal current collectors have garnered significant interest in the field of metallic Li as an ideal negative electrode. However, dendritic Li growth creates unoccupied space in the battery, diminishing volumetric energy density. Our research reveals that Li adatoms can reposition on metal substrates via surface migration by interacting with individual grains at the atomic level after electro-adsorption of Li ions. By examining Li morphologies on diverse types of substrates, we find that the near-zero migration barrier of Li adatoms, especially on single crystal Cu(111) foils, is a key parameter that inhibits Li dendrites by initiating horizontal growth in an isotropically faceted nucleation shape, with 80% capacity retention even after 120 cycles (versus 29 cycles for polycrystalline Cu), paired with LiNi0.8Co0.1Mn0.1O2 (NCM811) cathodes with a high-loading level (5.3 mA h cm−2). Based on our findings, we highlight the importance of metal substrates that promote favorable surface dynamics of Li adatoms.
27 September 2026 in Advanced Science
Lithiation in graphite electrodes proceeds heterogeneously, yet how this heterogeneity develops in space, and how it responds to the kinetic conditions of charging, remains poorly resolved because conventional probes report only volume‐averaged behavior. Here we resolve how graphite staging heterogeneity evolves across both the through‐thickness and in‐plane directions of the electrode, and how its severity is governed by charging kinetics. Combining operando optical microscopy, in situ x‐ray diffraction, color‐space analysis, and electrode‐scale simulation, we track lithiation from the particle scale to the full electrode as a function of electrode porosity and charging rate. Lower porosity and higher rate intensify tortuosity‐controlled Li + transport limitation, generating through‐thickness lithiation gradients that evolve into pronounced in‐plane staging non‐uniformity, such that neighboring regions advance through the staging sequence at markedly different rates. Critically, operando imaging directly reveals that domains reaching advanced lithiation states earliest become the preferential sites at which lithium plating initiates, demonstrating that plating is spatially templated by pre‐existing staging heterogeneity rather than nucleating randomly. These findings establish staging heterogeneity as a kinetically controlled precursor to plating and provide a general operando framework for diagnosing heterogeneity‐driven behaviour in insertion electrodes.