Polarization reversal in polycrystalline ferroelectrics is shown to occur via two distinct and sequential domain reorientation steps. This reorientation sequence, which cannot be readily discriminated in the overall sample polarization, is made apparent using time-resolved high-energy x-ray diffraction. Upon application of electric fields opposite to the initial poling direction, two unique and significantly different time constants are observed. The first (faster time constant) is shown to be derived by the release of a residual stress due to initial electrical biasing and the second (slower time constant) due to the redevelopment of residual stress during further domain wall motion. A modified domain reorientation model is given that accurately describes the domain volume fraction evolution during the reversal process.
With high power light emitting diodes and laser diodes being explored for white light generation and visible light communication, thermally robust encapsulation schemes for color-converting inorganic phosphors are essential. In the current work, the canonical blue-emitting phosphor, high purity Eu-doped BaMgAl10O17, has been prepared using microwave-assisted heating (25 min) and densified into translucent ceramic phosphor monoliths using spark plasma sintering (30 min). The resulting translucent ceramic monoliths convert UV laser light to blue light with the same efficiency as the starting powder and provide superior thermal management in comparison with silicone encapsulation.
SiAlON ceramics, solid solutions based on the Si3N4 structure, are important, lightweight structural materials with intrinsically high strength, high hardness, and high thermal and chemical stability. Described by the chemical formula β-Si6–zAlzOzN8–z, from a compositional viewpoint, these materials can be regarded as solid solutions between Si3N4 and Al3O3N. A key aspect of the structural evolution with increasing Al and O (z in the formula) is to understand how these elements are distributed on the β-Si3N4 framework. The average and local structural evolution of highly phase-pure samples of β-Si6–zAlzOzN8–z with z = 0.050, 0.075, and 0.125 are studied here, using a combination of X-ray diffraction, NMR studies, and density functional theory calculations. Synchrotron X-ray diffraction establishes sample purity and indicates subtle changes in the average structure with increasing Al content in these compounds. Solid-state magic-angle-spinning 27Al NMR experiments, coupled with detailed ab initio calculations of NMR spectra of Al in different AlOqN4–q tetrahedra (0 ≤ q ≤ 4), reveal a tendency of Al and O to cluster in these materials. Independently, the calculations suggest an energetic preference for Al–O bond formation, instead of a random distribution, in the β-SiAlON system.
21 September 2017 in Journal of Materials Chemistry C
Inorganic phosphor materials play a crucial role in the creation of white light from blue and near-UV solid-state light-emitting diodes. Understanding the intricacies of the phosphor structure is key for setting the stage for improved, more efficient functionality. Average structure and coordination environment analysis of the robust and efficient green-emitting phosphor, β-SiAlON:Eu2+ (β-Si6−zAlzOzN8−zEu0.009), is combined here with a range of property measurements to elucidate the role of Al content (z) in luminescence properties, including the red shift of emission and the thermal quenching of luminescence as a function of increasing Al content z. Average structure techniques reveal changes in polyhedral distortion with increasing z for the 9-coordinate Eu site in β-SiAlON:Eu2+. X-ray absorption near edge structure (XANES) is used to confirm that the majority of the activator Eu is in the Eu2+ state, exhibiting the symmetry-allowed and efficient 4f75d0 → 4f65d1 transitions. Room temperature and temperature-dependent luminescence indicate a curious increase in thermal stability with increasing z over a small range due to an increasing barrier for thermal ionization, which is correlated to an increase in the quantum yield of the phosphor.