Surface treatment, using two slurries containing nanomaterials, was applied to recycled aggregate (RA). Experimental studies were conducted (1) to compare properties of RA before and after the surface treatment; and (2) to examine the modification effects of the surface treatment with nanomaterials on the microstructure and macroproperties of recycled aggregate concrete (RAC). The nanoindentation technique was used to achieve elastic modulus of different interface transition zones (ITZs) and old and new mortars in RAC. Test results show that both nanoslurries enhanced new ITZs between the old and new cement mortars. Although they did not work on old ITZs between the virgin aggregate and the old cement mortar, old mortars were surface strengthened. It is also proved that properties of both RA and RAC on the macroscale were improved by the surface treatment using nanomaterials.
1 October 2006 in Advances in Structural Engineering
This article tries to contribute to quantify the amount of steel corrosion at the cracking of concrete cover. The amount of steel corrosion when the concrete cover cracks, is a key factor in the life of concrete structures. During the time between steel depassivation and concrete cover cracking, the process of steel corrosion develops in three stages: free expansion of the corrosion products, stress initiation of the concrete cover, and cracking of the concrete cover. A concrete cracking model is presented here to estimate the total amount of steel corrosion at the onset of the cracking of the concrete cover. This model is applied to some test results reported by other researchers. The amount of steel corrosion predicted by the proposed model when cracking of the concrete cover occurs is in agreement with the experimentally observed results.
20 December 2024 in Construction and Building Materials
In this study, the effect of corrosion on the static behavior of stud shear connectors was investigated. Two series of push test specimens having different stud diameters were fabricated according to Eurocode 4. The test specimens were first corroded to different corrosion rates by electronic accelerating method. Static loading tests were then performed to obtain the load-slip curves and ultimate strengths of corroded test specimens. Material properties of the concrete and steel studs used in the test specimens were also measured. Actual corrosion rates were measured from the studs obtained from the tested specimens. Design methods specified in current design standards are used to predict the design strengths of test specimens. It is shown that the design strengths are unconservative for corroded test specimens. Therefore, a new design equation is proposed which enables the designer to consider the effect of corrosion.