2 March 2012 in Optical Materials Express
AIAdrián Itzmoyotl-Toxqui
We report the study of hydrogenated amorphous silicon-germanium (a-Si1-XGeX:H) films prepared by low-frequency plasma-enhanced chemical vapor deposition (LF-PECVD) varying the composition (0 ≤ X ≤ 1). Silicon and germanium content is determined by energy dispersion spectroscopy (EDS). Refractive index, absorption coefficient and optical gap are estimated by transmittance measurements as well as by the use of PUMA software. Absorption coefficients obtained by using this software and by the Beer-Lambert law show good agreement according to absorption region. Results indicate that refractive index exhibits a linear behavior on germanium content for atomic percent (at.%). Employing these films and by the use of the finite-element software COMSOL, a single-mode low-contrast rib optical waveguide operating at the wavelength of 1550 nm is simulated, and later fabricated by using photolithography and plasma etching techniques. Measured optical losses are 7.6 dB/cm.
1 December 2019 in AIP Advances
This work proposes and demonstrates the concept of a complementary metal-oxide-semiconductor (CMOS)-compatible electrophotonic monolithic refractive index sensor in which a Si-based light source is directly integrated. The device consists of an embedded light emitter, a waveguide, a sensing area to place an analyte, and a photodetector. The behavior of the system was modeled and simulated using light propagation and semiconductor simulation software. Experimental devices were fabricated using all standard CMOS materials and procedures, and the tests showed changes in detected photocurrent related to the refractive index of the material in the sensing area, demonstrating the potential of the completely Si-based CMOS-compatible electrophotonic systems in the development of fully integrated sensors.
30 December 2016 in Journal of Vacuum Science & Technology B
AIAdrián Itzmoyotl-Toxqui
Silicon films with subwavelength structures were prepared on flexible polyimide by plasma deposition. Resulting films exhibited high photosensitivity and high stability. The varied parameters were pressure and silane (SiH4) flow, while power, frequency, temperature, and hydrogen (H2) flow were fixed. Pressure was set at 0.7 or 1.3 Torr, while the SiH4 flow rate was set at 10, 50, or 100 sccm. Similar characteristics were observed for the films when the same SiH4 flow rate was used, despite pressure variations. Deposition rate from 0.94 to 5.86 Å/s, optical gap from 1.6 to 2 eV, and embedded nanocrystals in the range of 2–6 nm were the main characteristics of our films. Subwavelength structures from 102 to 287 nm in diameter were observed. These structures scatter the photons and thus improve absorptance, photosensitivity, and mobility-lifetime product. The structural and optoelectronic properties of these films showed a high correlation with the silane concentration obtained from the partial pressure of SiH4 and H2.
1 March 2024 in Journal of Vacuum Science & Technology B
In this work, the synthesis of germanium-tin (GeSn) films by magnetron sputtering is reported. A fractional factorial experiment was conducted; the varied factors were temperature, power applied to Ge target by a radio-frequency source, and power applied to the Sn target by a direct-current source. Vibrational modes, film composition, morphology, deposition rate, dark conductivity, Raman spectra, and Fourier-transform infrared (FTIR) spectra of the GeSn films were analyzed. Mid-infrared spectrum of emission and absorption was obtained by FTIR electroluminescence (EL) spectroscopy in the range of 400–4000cm−1, thermal emission was monitored by a FLIR camera in the range of 8–14μm, and power emitted from the GeSn films was measured in the range of 2.7–5.3μm by means of a InAsSb photodetector; results obtained by these approaches at room temperature and low-field bias were consistent. Sample Ge0.71Sn0.29 exhibited Ge Raman crystalline fraction of 85%; from FTIR EL spectrum were observed peaks of absorption located at 1084, and 606 cm−1 that was attributed to Si−Si bonds from the c-Si substrate, as well as broadband attenuation of 2% in the range of 1500−3500cm−1, this behavior was associated to the self-heating of this sample at 90 °C. Sample Ge0.3Sn0.7 showed Raman crystalline fraction of 16 and 22% for Ge and Sn, respectively; from FTIR EL spectrum were observed peaks of emission located at 2.74 μm (0.452 eV) and 6.66 μm (0.186 eV), as well as broadband emission in the range of 600–2000 cm−1 attributed to Planck’s law at a temperature of 45 °C; these results were correlated to the proper content of Ge and Sn, fluctuating current, and polymorphic morphology of this sample.
14 April 2016 in MRS Proceedings
FHFrancisco J. De la Hidalga-Wade
Francisco J. De la Hidalga-Wade
AIAdrián Itzmoyotl-Toxqui
23 October 2025 in Infrared Physics & Technology