20 December 2021 in npj Materials Degradation
Standard methods to assess the durability of vitrified radioactive waste were first developed in the 1980’s and, over the last 40 years, have evolved to yield a range of responses depending on experimental conditions and glass composition. Mechanistic understanding of glass dissolution has progressed in parallel, enhancing our interpretation of the data acquired. With the implementation of subsurface disposal for vitrified radioactive waste drawing closer, it is timely to review the available standard methodologies and reflect upon their relative advantages, limitations, and how the data obtained can be interpreted to support the post-closure safety case for radioactive waste disposal.
3 April 2019 in npj Materials Degradation
Radioactive waste immobilization is a means to limit the release of radionuclides from various waste streams into the environment over a timescale of hundreds to many thousands of years. Incorporation of radionuclide-containing wastes into borosilicate glass during vitrification is one potential route to accomplish such immobilization. To facilitate comparisons and assessments of reproducibility across experiments and laboratories, a six-component borosilicate glass (Si, B, Na, Al, Ca, Zr) known as the International Simple Glass (ISG) was developed by international consensus as a compromise between simplicity and similarity to waste glasses. Focusing on a single glass composition with a multi-pronged approach utilizing state-of-the-art, multi-scale experimental and theoretical tools provides a common database that can be used to assess relative importance of mechanisms and models. Here we present physical property data (both published and previously unpublished) on a single batch of ISG, which was cast into individual ingots that were distributed to the collaborators. Properties from the atomic scale to the macroscale, including composition and elemental impurities, phase purity, density, thermal properties, mechanical properties, optical and vibrational properties, and the results of molecular dynamics simulations are presented. In addition, information on the surface composition and morphology after polishing is included. Although the existing literature on the alteration of ISG is not extensively reviewed here, the results of well-controlled static alteration experiments are presented here as a point of reference for other performance investigations.
10 September 2018 in npj Materials Degradation
Assessment of glass dissolution kinetics, under disposal relevant temperature and pH environments, is required to credibly estimate radionuclide release rates from vitrified radioactive waste. Leaching of the International Simple Glass (ISG) under acidic to hyperalkaline conditions was examined. Forward rate measurements have been obtained using the dynamic leaching SPFT protocol and rate parameters for B, Na and Si in the basic regime; errors in rates predicted using these parameters at high pH and temperature are significant because the fitting uses logarithmic data. Longer term behaviour under hyperalkaline conditions, representative of some disposal environments, was investigated using the PCT and MCC-1 static leaching protocols with Ca(OH)2 solutions for up to 120 days (PCT) and 720 days (MCC-1). In hyperalkaline conditions dissolution was incongruent for all elements and the presence of alternating zirconia-rich and zirconia-poor alteration layers was observed on all leached monoliths, indicating the occurrence of a self-organisation phenomenon during leaching.
1 October 2016 in Journal of Nuclear Materials
The UK high level nuclear waste glass modified with CaO/ZnO was investigated using the vapour phase hydration test, performed at 200 °C, with the aim of understanding the impact of the modification on the chemical composition and microstructure of the alteration layer. Experiments were undertaken on non-modified and CaO/ZnO-modified base glass, with or without 25 wt% of simulant Magnox waste calcine. The modification resulted in a dramatic reduction in gel layer thickness and also a reduction in the reaction rate, from 3.4 ± 0.3 g m−2 d−1 without CaO/ZnO modification to 0.9 ± 0.1 g m−2 d−1 with CaO/ZnO. The precipitated phase assemblage for the CaO/ZnO-modified compositions was identified as hydrated Ca- and Zn-bearing silicate phases, which were absent from the non-modified counterpart. These results are in agreement with other recent studies showing the beneficial effects of ZnO additions on glass durability
1 October 2002 in International Journal of Fatigue
5 October 2007 in Journal of Environmental Monitoring
A slag sample from a lead refiner has been obtained and given to two analytical laboratories to determine the release of trace elements from the sample according to BS EN 12457-2. Samples analysed by one laboratory passed waste acceptance criteria, leading it to be classified as an inert material; samples of the same material analysed by the other laboratory failed waste acceptance criteria and were classified as hazardous. It was found that the sample preparation procedure is the critical step in the leaching analysis and that the effects of particle size on leachability should be taken into account when using this standard. The purpose of this paper is to open a debate on designing a better defined standard leaching test and making current waste acceptance criteria more flexible.