In the implantation of porous bone scaffolds, good mechanical properties of the scaffold are a prerequisite for the long-term functionality of the implanted scaffolds, which varies according to the structure and the forming process. In this study, the influence of the forming parameters and structure of the Selective Laser Melting (SLM) process on the mechanical properties of 316L stainless steel bone scaffolds was investigated using finite element simulation combined with experimental methods. The mechanism of the influence of the process parameters and structure on the mechanical properties of bone scaffolds was summarized using static compression finite element numerical simulations, compression experiments, hydrodynamic simulations, forming numerical simulations and SLM forming experiments. The results show that the magnitude of residual stress and the distribution of defects under different process parameters had a strong influence on the microstructure and properties of the scaffold, and the residual stress of the Body-Centered Cube (BCC) structure formed at an energy density of 41.7 J/mm3 was significantly reduced, with less surface spheroidization and fewer cracks on the melt pool surface. The smallest grain size of 321 nm was obtained at an energy density of 77.4 J/mm3, while in terms of mechanical properties, the optimization of the structure resulted in an 8.3% increase in yield strength and a reduction in stress concentration. The predictions of stress, deformation, and forming quality during construction with different process parameters, achieved using finite element analysis, are basically in agreement with the experimental results, indicating that the best process parameters for forming BCC structural supports were determined by using finite element simulation combined with experiments; moreover, the distribution and evolution of residual stresses and defects under different process parameters for constructing BCC structures were obtained.
17 September 2021 in International Journal of Applied Ceramic Technology
Thick TA1 titanium alloy sheets were thoroughly bonded by vacuum electron beam welding (EBW). The results indicated that microstructures in the weld zone (WZ) consisted of coarse α columnar grains, serrated α as well as needle-shaped α ′; the microstructure in the heat-affected zone near the WZ side was composed of α ′ and α , while the microstructure near the base metal side consisted of α ″ and α . The positional relation between the notches and rolling direction had an important role in the impact performance. The EBW joint exhibited higher absorbed impact energy at the weld seam after local heat treatment. Furthermore, lots of dimples were produced on the impact fracture surfaces, exhibiting ductile fractures.