23 August 2017 in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
In France, the reference concept for the geological disposal of high-level waste (HLW) consists of horizontal micro-tunnels, containing carbon steel casing and overpacks (around a stainless steel container containing vitrified waste). The overpacks and casing will be exposed to an environment that will evolve over time: from a hot and humid atmosphere containing oxygen, to an anoxic environment saturated with water at the geothermal temperature. Lots of corrosion experiments have been performed in representative environments to study steel corrosion modes (general corrosion, pitting and crevice corrosion, stress corrosion cracking, hydrogen embrittlement…) while taking into account the influence of temperature, radiation, mechanical stresses and microorganisms. Some key results have influenced the design of the HLW disposal cell, including the carbon steel grades and dimensions of the casing and overpacks, or the addition of an alkaline grout material between the casing and the host rock. This paper is part of a supplement on the 6th International Workshop on Long-Term Prediction of Corrosion Damage in Nuclear Waste Systems .
21 February 2017 in Swiss Journal of Geosciences
Carbon steel is widely considered as a candidate material for the construction of spent fuel and high-level waste disposal canisters. In order to investigate corrosion processes representative of the long term evolution of deep geological repositories, two in situ experiments are being conducted in the Mont-Terri rock laboratory. The iron corrosion (IC) experiment, aims to measure the evolution of the instantaneous corrosion rate of carbon steel in contact with Opalinus Clay as a function of time, by using electrochemical impedance spectroscopy measurements. The Iron Corrosion in Bentonite (IC-A) experiment intends to determine the evolution of the average corrosion rate of carbon steel in contact with bentonite of different densities, by using gravimetric and surface analysis measurements, post exposure. Both experiments investigate the effect of microbial activity on corrosion. In the IC experiment, carbon steel showed a gradual decrease of the corrosion rate over a period of 7 years, which is consistent with the ongoing formation of protective corrosion products. Corrosion product layers composed of magnetite, mackinawite, hydroxychloride and siderite with some traces of oxidising species such as goethite were identified on the steel surface. Microbial investigations revealed thermophilic bacteria (sulphate and thiosulphate reducing bacteria) at the metal surface in low concentrations. In the IC-A experiment, carbon steel samples in direct contact with bentonite exhibited corrosion rates in the range of 2 µm/year after 20 months of exposure, in agreement with measurements in absence of microbes. Microstructural and chemical characterisation of the samples identified a complex corrosion product consisting mainly of magnetite. Microbial investigations confirmed the limited viability of microbes in highly compacted bentonite.
28 April 2017 in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
This paper presents a state-of-the-art analysis of the expected degradation processes of a variety of candidate container materials for the disposal of high-level waste and/or spent nuclear fuel. The work, focusing on the most recent developments, has been performed under the auspices of the Implementing Geological Disposal Technology Platform in the context of an international conference hosted by the Nuclear Waste Management Organisation of Canada (NWMO). The scope of the analysis includes the expected corrosion and environmentally assisted cracking behaviour of copper, carbon steel and titanium in contact with relevant buffer materials (e.g. bentonite, cement) and in conditions expected in an underground disposal facility (long-term anoxic conditions). Considerations relative to the expected evolution of the environmental conditions (especially in the period following backfilling) are also presented. Beyond summarising the current state of knowledge, areas in which opportunities for international collaboration may be present are also highlighted. This paper is part of a supplement on the 6th International Workshop on Long-Term Prediction of Corrosion Damage in Nuclear Waste Systems.
1 November 2015 in Electrochimica Acta
28 April 2017 in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
In the context of the French repository for high-level wastes, carbon steel (C-steel) materials are currently considered among the most cost effective and reliable materials for the prediction of long-term corrosion behaviour. An in situ experiment was conducted at the Meuse/Haute Marne underground research laboratory to investigate the corrosion behaviour of different grades of C-steel up to a maximum temperature of 85°C. C-steel coupons were placed in a two-phase test chamber containing liquid and gas emanating from the Callovo-Oxfordian host rock, at given times and for specific durations, under anoxic conditions. After their exposure in the test chamber, various characterisations were carried out. Overall, after 36 months, the results highlight a potential acidic transient. This could promote high corrosion rates of C-steel. Therefore, an alternative concept has been considered since 2014, which involves the addition of a cement–bentonite-based grout in order to buffer the possible acidic transient. This paper is part of a supplement on the 6th International Workshop on Long-Term Prediction of Corrosion Damage in Nuclear Waste Systems.
28 April 2017 in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
The French national radioactive waste management agency (Andra) is in charge of studying the disposal of high level wastes (HLW) in deep geological repositories. The reference concept for HLW disposal cells consisted of a multi-barrier system: horizontal boreholes drilled in the Callovo Oxfordian (COx) claystone, cased with carbon steel (C-steel) and containing C-steel overpacks with the nuclear waste packages. Mechanical strength is required for the metallic structures to ensure safety. This study presents the work performed on C-steel to assess in situ mechanical loading, long-term mechanical behaviour based on modelling and environmentally assisted cracking (EAC) susceptibility. The results from in situ experiments have demonstrated anisotropy of the mechanical loading of the casing. Long-term calculations revealed local plastic strain after a few years to a few decades, which highlighted the need to assess the potential risk of EAC. Eventually, the results on EAC assessment in the COx claystone confirmed that the microstructure of the casing and overpack plays a key role on the mechanical resistance. This paper is part of a supplement on the 6th International Workshop on Long-Term Prediction of Corrosion Damage in Nuclear Waste Systems.