Terrassa Institute of Textile Research and Industrial Cooperation (INTEXTER), Universitat Politècnica de Catalunya-BarcelonaTech (UPC), Terrassa, Spain
Auto-generated profile, based on publicly available information
Ines Algaba
Terrassa Institute of Textile Research and Industrial Cooperation (INTEXTER), Universitat Politècnica de Catalunya-BarcelonaTech (UPC), Terrassa, Spain
Raw hemp fibers are alkaline delignified to evaluate the effect of lignin on the moisture uptake behavior of hemp. Samples are subjected to moisture absorption/desorption isotherms from 5% to 95% relative humidity at three different temperatures (15, 25, and 35°C). The sorption ratio between delignified and untreated hemp is lowered by 25%. Hysteresis makes evident the greater influence of lignin on moisture binding at low relative humidity while at high relative humidity, cellulose plays the most important role. The GAB, Hailwood‐Horrobin and Dent models are fitted to absorption/desorption isotherms. Delignification and temperature decrease the size of the monolayer. The energy constants of the monolayer differ according to the model used. Lignin causes great differences between absorption and desorption. The greater the temperature is, the lower the monolayer energy constant. The energy constants of the multilayer are identical for the three models, showing a greater range of variation in delignified samples than in the untreated samples. Based on primary and secondary energy constants, bonding enthalpies are determined. Estimations in desorption show higher correlation coefficients with the energy constants, which enables to conclude that measures in desorption better explain the effect of delignification on the water uptake behavior of hemp.
This research focused on establishing the spinning potential of non-textile hemp by using mechanical-chemical cottonization. The raw material used was an agricultural residue that is mainly employed for paper manufacturing. These fibers were subjected to an alkaline chemical treatment followed by an oxidizing treatment (H2O2) to reduce non-cellulosic components. Subsequently, a mechanical process was carried out to increase fiber elementarization and obtain suitable slivers for spinning. The potential of open-end rotor spinning was evaluated for both the 100% treated hemp and blends of 25% hemp/75% cotton. The selection criteria included a low reduction of the degree of cellulose polymerization, a low mass loss during the process, an appropriate tensile strength of the resulting yarns, an absence of breakage during spinning, and a low twist. The hemp treated with a high level of H2O2 stabilizer, according to the established experimental design for the oxidizing process, exhibited superior performance when blended with cotton and spun with a count of 40 tex and a twist coefficient (αm) of 170. These outcomes are of industrial interest for the production of fine yarns because they can be easily implemented using existing machinery devoted to processing cotton. Furthermore, it contributes to the circular economy within the textile industry by adding value to a waste material that can serve as an alternative source of more environmentally friendly cellulosic fibers. Graphical abstract