2,3-Dialdehyde cellulose (DAC) of a high degree of oxidation (92% relative to AGU units) prepared by oxidation of microcrystalline cellulose with sodium periodate (48 °C, 19 hours) is soluble in hot water. Solution casting, slow air drying, hot pressing and reinforcement by cellulose nanocrystals afforded films (~100 µm thickness) that feature intriguing properties: they have very smooth surfaces (SEM), are highly flexible and have good light transmittance for both the visible and near-infrared range (89-91%), high tensile strength (81-122 MPa) and modulus of elasticity (3.4-4.0 GPa) depending on hydration state and respective water content. The extraordinarily low oxygen permeation of < 0.005 cm3 µm m-2 d-1 kPa-1 (50 % RH) and < 0.03 cm3 µm m-2 d-1 kPa-1 (80 % RH) can be regarded as a particularly interesting feature of DAC films. The unusual high initial contact angle of about 67° revealed a rather low hydrophilicity compared to other oxidatively modified or unmodified cellulosic materials which is most likely the result of inter- and intramolecular hemiacetal and hemialdal formation during drying and pressing.
Recently, a new member of the nanocellulose family was introduced, a cellulose II gel consisting of nanostructured and spherical particles. In this study, we compared two different drying techniques to obtain highly porous powders from this gel with preserved meso- and macroporous nanostructure: first, freeze-drying after solvent exchange to tBuOH and second, supercritical drying of the respective EtOH alcogel. The approaches yielded aerogel powders with surface areas of 298 and 423 m2/g, respectively. Both powders are amphiphilic and possess energetically heterogeneous surfaces with dominating dispersive term of the surface energy in the range of 50–52 mJ/m2, as determined by a combination of physicochemical surface characterization techniques, such as iGC, BET and SEM. Despite the lower surface area, the cheaper and more widespread method, freeze-drying, yields a more polar and reactive cryogel.