Department of Chemistry and Chemical Engineering, Chalmers University of Technology, Gothenburg, SE-412 96, Sweden; FibRe Centre for Lignocellulose-based Thermoplastics, Chalmers University of Technology, Gothenburg, SE-412 96, Sweden
Auto-generated profile, based on publicly available information
Ratchawit Janewithayapun
Department of Chemistry and Chemical Engineering, Chalmers University of Technology, Gothenburg, SE-412 96, Sweden; FibRe Centre for Lignocellulose-based Thermoplastics, Chalmers University of Technology, Gothenburg, SE-412 96, Sweden
Arabinoxylan (AX) with varying arabinose to xylose (A/X) ratios of 0.85, 0.57 and 0.39 was extracted from wheat bran, and the conformations of the AX polysaccharides dispersed in water were investigated using small-angle X-ray scattering. The persistence length (Lp) and the conformation statistics (expressed by the Flory exponent v or the mass fractal) of the AX varied with their A/X ratios. The Lp decreased with decreasing A/X ratio, from 4.5 nm to 1.5 nm, where the AX with high and intermediate A/X ratios can be considered semi-flexible chains, while AX with the lowest A/X ratio behaves as a flexible chain. The mass fractal increased from 1.7 to 2.5 between the highest and lowest A/X ratios, indicating increasingly compact polymer conformations. AX with the highest A/X ratio behaved as chains in a good solvent and was well dispersed even in the semi-dilute regime. AX with intermediate and low A/X ratios showed stronger tendencies to aggregate and were not well dispersed at higher concentrations. The results presented show that the macroscopic properties of AX dispersions can be understood based on the chemical composition and fine structure of the AX polysaccharide.
The effect of periodate oxidation and borohydride reduction on arabinoxylan (AX) in aqueous solution was investigated using 13C NMR spectroscopy and small-angle X-ray scattering (SAXS). AX consists of a xylose backbone, which is mono- or di-substituted with arabinose. We show that at a ring-opening modification degree of 21%, periodate oxidation occurs predominantly on arabinose, and shows a preference for arabinose linked to di-substituted xylose units over the mono-substituted. With a higher degree of modification of 33%, arabinose at the mono-substituted position and unsubstituted xylose units are also modified. At 33% a large portion of oxidizable AX residues have been ring-opened, yet SAXS reveals no significant changes in chain conformation and only a minor reduction (10%) in persistence length for the oxidized-reduced dialcohol AX. With increasing degree of oxidation, dialdehyde AX instead show an increasing tendency for aggregation, attributed to chain cross-linking. Upon reduction of the dialdehyde and cross-linked groups to dialcohol AX, the chains revert back to having repulsive interactions, acting as chains in a good solvent environment.
Nanocelluloses are uniquely valued for their high surface area and controllable assembly. This study elucidates the assembly of cellulose nanocrystals (CNCs) in tert-butanol (TBA) and water mixtures. We emphasize the influence of TBA on the structure of suspensions and freeze-dried foams. Although the length-scale of CNC organization is large relative to water-TBA structures, adding more than 30 wt % TBA shifted ordered CNC packing into an isotropic network. The change was attributed to the disruption of ionic interactions and adsorption of TBA to hydrophobic CNC interfaces; manifesting as a 5-fold increase in viscosity at 50 wt % TBA content. The freeze-dried foams' morphology was transformed due to TBA-modulated crystal growth during the freezing process. This led to the intriguing capability to control foams' mechanical strength and surface area, achieving up to 3 and 15-fold increases, respectively. The investigations highlight TBA's potential as a structuring agent in solvent-mediated design of nanomaterial systems.